load deflection characteristics of nickel titanium initial archwires

نویسندگان

hossein aghili

sogra yasssaei

mahmoud nilli ahmadabadi

neda joshan

چکیده

objectives: the aim of this study was to assess and compare the characteristics of commonly used initial archwires by their load deflection graphs. materials and methods : this study tested three wire designs namely copper nickel titanium (cnt), nickel titanium (niti), and multi-strand niti (msnt) archwires engaged in passive self-ligating (psl) brackets, active self-ligating (asl) brackets or conventional brackets. to evaluate the mechanical characteristics of the specimens, a three-point bending test was performed. the testing machine vertically applied force on the midpoint of the wire between the central incisor and canine teeth to obtain 2 and 4mm of deflection. the force level at maximum deflection and characteristics of plateau (the average plateau load and the plateau length) were recorded. two-way anova and tukey’s test were used at p <0.05 level of significance. results: force level at maximum deflection and plateau length were significantly affected by the amount of deflection. the type of archwires and brackets had significant effects on force level at maximum deflection, and plateau length. however, the bracket type had no significant effect on the average plateau force. conclusion: with any type of brackets in deflections of 2 and 4mm, msnt wire exerted the lowest while niti wire exerted the highest force level at maximum deflection and plateau phase. the force level at maximum deflection and the plateau length increased with raising the amount of primary deflection; however the average plateau force did not change significantly.

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Load Deflection Characteristics of Nickel Titanium Initial Archwires.

OBJECTIVES The aim of this study was to assess and compare the characteristics of commonly used initial archwires by their load deflection graphs. MATERIALS AND METHODS This study tested three wire designs namely copper nickel titanium (CNT), nickel titanium (NiTi), and multi-strand NiTi (MSNT) archwires engaged in passive self-ligating (PSL) brackets, active self-ligating (ASL) brackets or c...

متن کامل

Load-deflection characteristics of superelastic nickel-titanium wires.

OBJECTIVE To determine the mechanical properties of commercially available thermodynamic wires and to classify these wires mathematically into different groups. MATERIALS AND METHODS The samples examined were 48 nickel-titanium (NiTi) alloy orthodontic wires commercially available from five manufacturers. These samples included 0.016-inch, 0.016- x 0.022-inch, 0.017- x 0.025-inch, and 0.018- ...

متن کامل

Surface characteristics of retrieved coated and nickel-titanium orthodontic archwires.

OBJECTIVE The purpose of this study was to investigate the effects of oral fluids and archwire-bracket friction on the surface characteristics of NiTi alloy orthodontic archwires with/without aesthetic coating, in vivo for 2-3 months. MATERIALS AND METHODS Different cross-sections of NiTi Archwires (DENTSPLY GAC International) and Titanol Cosmetic Archwires (FORESTADENT® USA Inc.) were examin...

متن کامل

The effect of fluoride exposure on the load-deflection properties of superelastic nickel-titanium-based orthodontic archwires.

BACKGROUND It has been demonstrated that fluoride prophylactic agents may cause hydrogen absorption in NiTi wires and degrade their mechanical properties. AIMS To investigate the effect of a fluoride mouthwash on load-deflection characteristics of three types of nickel-titanium-based orthodontic archwires. METHODS Twenty maxillary 0.016 inch round specimens from each of the single-strand Ni...

متن کامل

Force-deflection properties of initial orthodontic archwires.

AIM This in vitro study measured the force-deflection behavior of selected initial alignment archwires by conducting three-point bending tests under controlled conditions. The study tested four wire designs: multistranded stainless steel, conventional stainless steel, superelastic nickel-titanium, and thermoactivated nickel-titanium archwires. METHOD The wires (n = 15) were ligated into stain...

متن کامل

Effect of Saliva on Load-Deflection Characteristics of Superelastic Nickel-Titanium Orthodontic Wires

OBJECTIVE Most published results about the characteristics of NiTi wires are based on the mechanical laboratory tests on the as-received wires.The purpose of this study was to investigate the effect of saliva on load-deflection characteristics of superelastic NiTi wires. MATERIALS AND METHODS In this experimental study, 15 wires of three kinds of superelastic NiTi wires (Sentalloy, Force I an...

متن کامل

منابع من

با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید


عنوان ژورنال:
journal of dentistry, tehran university of medical sciences

جلد ۱۲، شماره ۹، صفحات ۶۹۵-۷۰۴

میزبانی شده توسط پلتفرم ابری doprax.com

copyright © 2015-2023