comparison of shear bond strength of composite to stainless steel crowns using two mechanical surface treatments and two bonding systems

نویسندگان

sara ghadimi

alireza heidari

hamid sarlak

چکیده

objectives: this study aimed to compare the shear bond strength (sbs) of composite to stainless steel crowns (ssc) using two mechanical surface treatments (msts) and two bonding systems. materials and methods: eighty-four sscs were divided into six groups of 14; group1: no mst+scotchbond universal adhesive (n+u), group 2: surface roughening by a diamond bur+scotchbond universal adhesive (r+u), group 3: sandblasting+scotchbond universal adhesive (s+u), group 4: no mst+alloy primer+clearfil se primer and bond (n+a), group 5: surface roughening by a diamond bur+alloy primer+clearfil se primer and bond (r+a), group 6: sandblasting+alloy primer+clearfil se primer and bond (s+a). after mst and bonding procedure, composite cylinders were bonded to the lingual surface of sscs, then the sbs of composite to sscs was measured using a universal testing machine following thermocycling. results: the sbs of groups r+u and s+u was significantly higher than that of group n+u. no significant difference was noted in sbs of groups r+u and s+u. the sbs of group s+a was significantly higher than that of groups n+a and r+a. no significant difference was noted in the sbs of groups n+a and r+a (p>0.05). conclusions: in scotchbond universal adhesive groups, sandblasting and surface roughening by diamond bur significantly increased the sbs of composite to sscs compared to no mst. in alloy primer groups, sandblasting significantly increased the sbs of composite to ssc compared to surface roughening with diamond bur and no mst.

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Comparison of Shear Bond Strength of Composite to Stainless Steel Crowns Using Two Mechanical Surface Treatments and Two Bonding Systems

OBJECTIVES This study aimed to compare the shear bond strength (SBS) of composite to stainless steel crowns (SSC) using two mechanical surface treatments (MSTs) and two bonding systems. MATERIALS AND METHODS Eighty-four SSCs were divided into six groups of 14; Group1: No MST+Scotchbond Universal adhesive (N+U), Group 2: Surface roughening by a diamond bur+Scotchbond Universal adhesive (R+U), ...

متن کامل

In vitro evaluation of the effect of different surface treatments and bonding systems on shear bond strength of composite veneer to Stainless Steel Crown

Abstract   Background and aim: Using Stainless Steel Crowns (SSC) for Early Childhood Caries usually causes an unpleasant condition in the aesthetic of the patients. The aim of this study was to evaluate the effect of different surface treatments and bonding systems on shear bond strength of composite veneer to Stainless Steel Crown. Materials and Methods: In this in vitro study, 120 SSC were ...

متن کامل

Comparison of shear bond strength of the stainless steel metallic brackets bonded by three bonding systems

Introduction: In orthodontic treatment, it is essential to establish a satisfactory bond between enamel and bracket. After the self-etch primers (SEPs) were introduced for the facilitation of bracket bonding in comparison to the conventional etch-and-bond system, multiple studies have been carried out on their shear bond strengths which have yielded different results. This study was aimed at co...

متن کامل

Composite Bonding to Stainless Steel Crowns Using a New Universal Bonding and Single-Bottle Systems

Aim. The aim of this study is to evaluate the shear bond strength of nanocomposite to stainless steel crowns using a new universal bonding system. Material and Methods. Eighty (80) stainless steel crowns (SSCs) were divided into four groups (20 each). Packable nanocomposite was bonded to the lingual surface of the crowns in the following methods: Group A without adhesive (control group), Group ...

متن کامل

Shear Bond Strength of Nanocomposites to Dentin Substrate Treated with Er:YAG Laser Followed by Two Different Bonding Systems

Background and Aim: Preparation of tooth structure by laser systems produces a surface with different characteristics. Therefore, selecting an appropriate bonding system is necessary to achieve the maximum bond strength. The aim of this study was to compare the bond strength of Adper Single Bond 2 adhesive and Single Bond Univer-sal to dentin prepared by bur or laser. Materials and Methods: ...

متن کامل

comparison of shear bond strength between composite resin and porcelain using different bonding systems

statement of problem: ceramics as in ceramo-metallic and all ceramic tooth restorations have grown popular owing to their high tissue compatibility and esthetic advantages. such restorations have the capability to deliver valuable services over a long period of time; however, failures under intraoral conditions are not unanticipated. purpose: the purpose of this in-vitro study was to investigat...

متن کامل

منابع من

با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید


عنوان ژورنال:
journal of dentistry, tehran university of medical sciences

جلد ۱۳، شماره ۱، صفحات ۶۰-۶۷

میزبانی شده توسط پلتفرم ابری doprax.com

copyright © 2015-2023