study and analysis of al2o3-sic nanocomposite ceramics’ fracture toughness using vickers indenter

نویسندگان

alireza moradkhani

hamidreza baharvandi

mehdi tajdari

abbas vafaee sefat

چکیده

the basic trait in the ceramics is their high brittle or low fracture toughness, and the main criteria in the design and application is specifying the fracture toughness in ceramics. in this paper, a new method is proposed to determine the fracture toughness of ceramics, which is enhanced in lowering the cost of fracture toughness determination relative to the previous methods. hence due to the low cost and case of access of alumina (al 2 o 3 ) which is extensively used in ceramics industry, it is applied as the most important source for achieving the objectives. pure alumina has excellent properties such as refractory and high hardness on one hand, and has disadvantages such as low fracture toughness on the other hand. in order to improve its mechanical properties, various additives such as nano scale silicon carbide (sic) powder are used. in this paper, alumina micro powder having 5% nano magnesium oxide by weight were mixed separately with silicon carbide nano particles of 2.5%, 5%, 7.5%, 10% and 15% to construct various types of ceramics, with different physical and mechanical properties. semi experimental equation for their fracture toughness determination was presented and used for other brittle materials. this equation has minimal cost of experiments for determining fracture toughness of different brittle materials.

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Statistical Analysis of Vickers Indentation Fracture Toughness of Y-tzp Ceramics

The purpose of this study was to investigate and analyse the fracture toughness of yttria stabilized tetragonal zirconia polycrystal (Y-TZP) dental ceramics by means of the Vickers indentation technique. Fracture toughness was analysed under the following loads: 29.42 N, 49.03 N, 196.13 N, and 294.20 N. Cracks that had developed from the vertices of a Vickers indentation were measured and used ...

متن کامل

Fracture Toughness of Ceramics by the Vickers Indentation Crack Length Method: a Critical Review

Fracture toughness is an important property that characterizes a material’s brittleness or resistance to fracture. Although some fracture toughness test methods have been refined and even standardized, many researchers have continued to use the Vickers indentation crack length method as an expedient. In this paper, Vickers indentation fracture resistance data for Standard Reference Material SRM...

متن کامل

Determining the Toughness of Ceramics from Vickers Indentations Using the Crack-Opening Displacements: An Experimental Study

Recently, a method for evaluating the fracture toughness of ceramics has been proposed by Fett based on the computed crack-opening displacements of cracks emanating from Vickers hardness indentations. To verify this method, experiments have been conducted to determine the toughness of a commercial silicon carbide ceramic, Hexoloy SA, by measuring the crack-opening profiles of such Vickers inden...

متن کامل

Ultra-microhardness testing procedure with Vickers indenter

Depth-sensing indentation equipment is widely used for evaluation of the hardness and Young’s modulus of materials. The depth resolution of this technique allows the use of ultra-low loads. However, aspects related to the determination of the contact area under indentation should be cautiously considered when using this equipment. These are related to the geometrical imperfections of the tip, t...

متن کامل

Fracture toughness and thermal shock of tool and turbine ceramics

The behaviour of some commercial tool carbides and turbine ceramics has been investigated in regard to resistance to crack initiation, crack propagation and retained strength after thermal shock. New data are provided, particularly measurements of the fracture toughness of these materials at actual operating temperatures (up to 1200 ~ C). Many of the materials did not follow the generally accep...

متن کامل

Thermal-stress resistance and fracture toughness of two tool ceramics

The thermal-stress resistance and fracture strength behaviour of two oxide ceramics (a hot-pressed pure AI203 and a composite ceramic NTK-HC2) subjected to severe thermal shocks have been investigated. The damage resistance parameter (Kic/of)2 for both ceramics is also determined for a wide range of temperatures (25 ~ to 800 ~ C) and cross-head rates (10 -2 cm min -1 ~ 2.5 m sec -1 ). Fracture ...

متن کامل

منابع من

با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید


عنوان ژورنال:
international journal of advanced design and manufacturing technology

جلد ۴، شماره ۳، صفحات ۱-۱۱

میزبانی شده توسط پلتفرم ابری doprax.com

copyright © 2015-2023