biodegradable carboxymethyl cellulose films modified by polyvinyl alcohol and cellulose nanowhiskers:(1) structural and physical properties

نویسندگان

لیلا ابوالقاسمی

دانشجوی کارشناسی ارشد، دانشگاه تبریز بابک قنبرزاده

دانشیار، دانشگاه تبریز جلال دهقان نیا

استادیار، دانشگاه تبریز علی اکبر انتظامی

استاد شیمی، دانشگاه تبریز

چکیده

carboxymethyl cellulose (cmc)-polyvinyl alcohol (pvoh) blend film, containing 0-10% cellulose nanowhiskers (cnw), was produced through casting method, while physical properties of the films being investigated. cmc-pvoh-cnw nanocomposites, were prepared with a diluted suspension of cellulose nanowhiskers. nanowhiskers suspension was prepared through acid hydrolysis of cotton linter by sulfuric acid and contained rod like particles, averaging lengths of 240 nm and diameters of 13 nm. a 6.86% reduction in total moisture absorbency was achieved by a 10% wt pvoh addition to the cmc film. ultimate break tensile strength and strain increased by 19.25% and 12.21%, respectively, through an addition of 10% wt of pvoh. x-ray diffraction (xrd) test revealed uniform distribution of nanoparticles in biopolymer matrix. the addition of 10% wt cellulose nanowhiskers decreased the moisture absorption of the blend film while increasing the ultimate tensile strength of the film by 17.65% vs. 47.05%, respectively.

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

biodegradable carboxymethyl cellulose films modified by polyvinyl alcohol and cellulose nanowhiskers:(2) thermal, water vapor permeability and surface hydrophilicity properties

carboxymethyl cellulose (cmc)-polyvinyl alcohol (pvoh) blend film was produced through casting. cellulose nanowhisker (cnw) was produced by means of acid hydrolysis of cotton linter and cmc-pvoh-cellulose nanowhiskers through which fully degradable bionanocomposites were prepared. prepared nanowhisker suspension contained rod like particles averaging lengths of 240 nm and diameters of 13 nm. an...

متن کامل

Physical, Mechanical, and Antimicrobial Properties of Carboxymethyl Cellulose Edible Films Activated with Artemisia sieberi Essential Oil

Background: Edible films and coatings are biodegradable that can preserve the quality and extend the shelf life of foods. The aim of this study was to investigate the physical and mechanical properties, and antimicrobial activity of carboxymethyl cellulose (CMC) film containing Artemisia sieberi Essential Oil (AEO). Methods: The studied parameters were the antibacterial activity and physical p...

متن کامل

Effect of carboxymethyl cellulose concentration on physical properties of biodegradable cassava starch-based films

BACKGROUND Cassava starch, the economically important agricultural commodity in Thailand, can readily be cast into films. However, the cassava starch film is brittle and weak, leading to inadequate mechanical properties. The properties of starch film can be improved by adding plasticizers and blending with the other biopolymers. RESULTS Cassava starch (5%w/v) based films plasticized with glyc...

متن کامل

Synthesis, Characterisation and Flocculation Properties of Carboxymethyl Cellulose-g Acrylamide

Graft copolymers of acrylamide on carboxymethyl cellulose (d.s 0.4-0.5) were prepared by the use of ceric ion, ceric ion/reductant molecule initiator systems in aqueous medium. The graft copolymers were characterized by IR spectroscopy. The extent of graft copolymerisation was measured in terms of grafted chains as a function of both ceric ion and ceric ion/reductant molecule concentrations. It...

متن کامل

Electric Properties of Carboxymethyl Cellulose

Carboxymethyl cellulose [C6H7O(OH)3x(OCH2COOH)x]n is a derivative of the regenerated cellulose [C6H10O5]n with hydroxy-acetic acid (hydroxy ethanoic acid) CH2(OH)COOH or sodium monochloroacetate ClCH2COONa. The CMC backbone consist of D-glucose residues linked by -1,4-linkage. The molecular mass of one glucose unit in CMC chain is mCMC = 146.14 + 75.04x, where x  3 is the degree of substitu...

متن کامل

Compression properties of polyvinyl alcohol--bacterial cellulose nanocomposite.

Despite the established use of total joint replacement for the treatment of advanced degeneration of articular cartilage, component loosening due to wear and osteolysis limits the lifespan of these joint prostheses. In the present study, nanocomposites consisting of poly(vinyl alcohol) (PVA) and bacterial cellulose (BC) nanofibers were investigated as possible improved cartilage replacement mat...

متن کامل

میزبانی شده توسط پلتفرم ابری doprax.com

copyright © 2015-2023