hertzian load-bearing capacity of hybrid and nano-hybrid resin composites stored dry and wet

نویسندگان

s. farmani student research committee, shiraz dental school, shiraz university of medical sciences, shiraz, iran

s. orandi postgraduate student , department of prosthodontics, school of dentistry, shiraz university of medical sciences, shiraz, iran

m. sookhakiyan student research committee, shiraz dental school, shiraz university of medical sciences, shiraz, iran

ayse mese department of prosthodontics, school of dentistry, dicle university, diyarbakir, turkey

چکیده

abstract   statement of problem: hertzian indentation test has been proven to be an efficient and reliable alternative upon vickers hardness test. this method has been used to test dental ceramics, amalgams, glass ionomers and luting cements.there is limited published information about the load-bearing capacity of resin composites using hertizian indentation test. objectives: to investigate the load-bearing capacity of hybrid and nano-hybrid resin composites stored dry or wet up to 30 days, using hertzian indentation test. materials and methods: three resin composites were used: two nano-hybrids (filtek supreme, and luna) and one hybrid, (rok). a total of 108 disc-shaped specimens (1mm thick x 10 mm diameter) were prepared using polyethylene mould. the specimens of each material were randomly divided into 6 groups of 6 (n=6) and stored at 370c either in distilled water or dry for 1, 7 and 30 days. the specimens were tested using hertzian jig aligned in the universal testing machine. the specimen was placed on the top of a disc-shaped substrate. the load was applied at the center of each specimen and the load at the first crack was recorded. data were analyzed by anova, tukey’sand student’s t-test using spss version 18.0. results: three-way anova showed a significant interaction between all the factors (p = .0001). the load bearing capacity of almost all materials reduced significantly in the wet condition in comparison with the dry condition (p = .0001). after seven days of immersion in distilled water, filtek supreme had significantly lower values than those of rok and luna, there was no significant differences between materials in the dry condition. conclusions:in contrast to dry condition, the load-bearing capacity of specimens stored in distilled water decreased significantly over the 30 days of immersion. the load bearing capacity of nano-hybrid composites tested in this study was shown to be comparable with that of the hybrid composite.

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

fracture toughness of nanohybrid and hybrid composites stored wet and dry up to 60 days

statement  of  problem:  patients’ demand  for  tooth-colored  restoratives  in the posterior region is increasing. clinicians use universal nanohybrid resin composites for both anterior and posterior regions. there are few published reports comparing fracture toughness of nonohybrids and that of hybrid composite stored wet and dry. objectives: to investigate the fracture toughness of three nan...

متن کامل

Fracture Toughness of Nanohybrid and Hybrid Composites Stored Wet and Dry up to 60 Days

STATEMENT OF PROBLEM Patients' demand for tooth-colored restoratives in the posterior region is increasing. Clinicians use universal nanohybrid resin composites for both anterior and posterior regions. There are few published reports comparing fracture toughness of nonohybrids and that of hybrid composite stored wet and dry. OBJECTIVES To investigate the fracture toughness of three nanohybrid...

متن کامل

fracture toughness evaluation of hybrid and nano-hybrid resin composites after ageing under acidic environment

statement of problem: tooth-coloured restorative materials are brittle with the major shortcomings of sensitivity to flaws and defects. although various mechanical properties of resin composites have been studied, no fracture toughness test data for nano-hybrid composites under acidic condition for a long period of time has been published. objectives: to compare the fracture toughness (k ic ) o...

متن کامل

Electrical and Mechanical Performance of Hybrid and Non-hybrid Composites

This paper investigated the moisture absorption, mechanical behavior and the dielectric performance of hybrid and non-hybrid polymeric composites. Hand lay-up technique was used for processing carbon; glass reinforced polyester resin composites (non-hybrid) and carbon-glass/polyester hybrid composites with various fiber configurations. The maximum resistance of water absorption was obtained for...

متن کامل

Fabrication and Characterization of Nanostructured TiO2 and Turmeric Spent Incorporated Polystyrene Hybrid Nano Composites

A series of polystyrene hybrid nanocomposites have been fabricated with varying amounts of TiO2 viz., 0, 0.5 and 1 % w/w along with 3% TS by in-situ polymerization method. The influence of surface modified TiO2 nanoparticles on the thermal properties of PS matrix was examined using thermogravimetry and differential scanning calorimetry. Thermal characteristics of the polystyrene/TS/TiO2 hybrid ...

متن کامل

منابع من

با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید


عنوان ژورنال:
journal of dental biomaterials

جلد ۳، شماره ۱، صفحات ۱۶۲-۰

کلمات کلیدی
hertzian indentation load bearing capacity resin composites statement of problem hertzian indentation test has been proven to be anefficient and reliable alternative upon vickers hardness test. this methodhas been used to test dental ceramics amalgams glass ionomers and lutingcements.there is limited published information about the load bearingcapacity of resin composites using hertizian indentation test.objectives to investigate the load bearing capacity of hybrid andnano hybrid resin composites stored dry or wet up to 30 days using hertzianindentation test.materials and methods three resin composites were used two nano hybrids(filtek supreme and luna) and one hybrid (rok). a total of 108 disc shapedspecimens (1mm thick x 10 mm diameter) were prepared using polyethylene mould.the specimens of each material were randomly divided into 6 groups of 6(n=6) and stored at 370c either in distilled water or dry for 1 7 and 30 days.the specimens were tested using hertzian jig aligned in the universaltesting machine. the specimen was placed on the top of a disc shapedsubstrate. the load was applied at the center of each specimen and the loadat the first crack was recorded. data were analyzed by anova tukey’sandstudent’s t test using spss version 18.0.results three way anova showed a significant interaction between allthe factors (p = .0001). the load bearing capacity of almost all materialsreduced significantly in the wet condition in comparison with the drycondition (p = .0001). after seven days of immersion in distilled water filtek supreme had significantly lower values than those of rok and luna there was no significant differences between materials in the dry condition.conclusions in contrast to dry condition the load bearing capacity ofspecimens stored in distilled water decreased significantly over the 30 daysof immersion. the load bearing capacity of nano hybrid composites testedin this study was shown to be comparable with that of the hybrid composite.