Analysis of Surface Spalling on a First Intermediate Roll in Sendzirmir Mills

A first intermediate roll of Sendzirmir mills was failure by surface spalling during operation. After analyzing by visual, stereo microscope, optical microscope, scanning electron microscope, glow-discharged spectrometer and hardness test, respectively, the results show that some voids and cracks existed on the contact surface as well as subsurface. Further examination verified inadequate hardn...

متن کامل

Spectral Quasi-linearization for MHD Nanofluid Stagnation Boundary Layer Flow due to a Stretching/Shrinking Surface

This article concentrates on the effect of MHD heat mass transfer on the stagnation point nanofluid flow over a stretching or shrinking sheet with homogeneous-heterogeneous reactions. The flow analysis is disclosed in the neighborhood of stagnation point. Features of heat transport are characterized with Newtonian heating. The homogeneous-heterogeneous chemical reaction between the fluid and di...

متن کامل

Optimization of photo-degradation of direct blue 258 using nano Titanium Oxide with response surface method

The photodegradation of Direct Blue 258, a member of the group of azo dyes which are commonly used in the various branches of the industry, was studied. The photostability of this dye was not previously surveyed. Photocatalytic degradation method was evaluated. The both light source include solar simulated (UV 400 W lamp) and sun light (E= 400 W/m2) and titanium dioxide nanoparticles were used ...

متن کامل

Optimization of photo-degradation of direct blue 258 using nano Titanium Oxide with response surface method

The photodegradation of Direct Blue 258, a member of the group of azo dyes which are commonly used in the various branches of the industry, was studied. The photostability of this dye was not previously surveyed. Photocatalytic degradation method was evaluated. The both light source include solar simulated (UV 400 W lamp) and sun light (E= 400 W/m2) and titanium dioxide nanoparticles were used ...

متن کامل

Prediction of Work Roll Initial Crown according to Desired Strip Profile in Hot Rolling

The final hot strip profile is a superposition of the roll initial crown, the roll bending and flattening crown, the roll wearing crown and the roll thermal crown. In this research, linear regression models are proposed to predict the roll force, the roll wearing crown and the roll thermal crown using experimental data provided by Mobarake Steel Complex (MSC). The short beam theory based on ela...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: PAMM

سال: 2007

ISSN: 1617-7061,1617-7061

DOI: 10.1002/pamm.200701045