Low-Fusing Porcelain Glaze Application on 3Y-TZP Surfaces can Enhance Zirconia-Porcelain Adhesion.

The aim of this study was to assess whether surface treatment improves zirconia-porcelain adhesion. The 3Y-TZP blocks were cut into squares, then polished and sintered. The zirconia surface treatments were performed as follows: no treatment (C); tribochemical silica coating (TBS); glaze application + hydrofluoric acid etching (GA); glaze application + hydrofluoric acid etching + silanization (G...

متن کامل

Low temperature degradation of a Y-TZP dental ceramic.

Bars of Y-TZP ceramic for dental restorations were subjected to hydrothermal degradation via in vitro exposure to water steam at 140°C for 7 days. X-ray diffraction, atomic force microscopy and scanning electron microscopy techniques were applied to observe and quantify the tetragonal-monoclinic (t-m) phase transformation associated with the process. Nanoindentation was used to assess the ceram...

متن کامل

Evaluation of resin bond strength to yttria-stabilized tetragonal zirconia and framework marginal fit: comparison of different surface conditionings.

The purpose of this study was to evaluate the effect of different surface treatments of yttria-stabilized tetragonal zirconia (Y-TZP) on bond strength durability and marginal discrepancies. For adhesion testing, 144 specimens of VITA In-Ceram YZ ceramic for InLab were obtained (5.25×3.75×4.5 mm) and divided into six groups (n=24) according to the surface treatment: 1) Control (CRTL): untreated;...

متن کامل

Fracture Resistance and Surface Treatment of Y-tzp Prepable Ceramic Abutments and Bars

NIMET DIAMOND ADATIA Fracture Resistance And Surface Treatment Of Y-TZP Prepable Ceramic Abutments and Bars. (Under the direction of Dr. Stephen Bayne) Intraoral preparation of zirconia implant abutments creates deep surface defects making abutments susceptible to fracture during loading. Fracture strengths were tested for (1) HIP-processed zirconia bars (Astra-Tech) after preparation and/or su...

متن کامل

Deposition of Crystalline Hydroxyapatite Nanoparticles on Y-TZP Ceramic: A Potential Solution to Enhance Bonding Characteristics of Y-TZP Ceramics

Objectives Many advantages have been attributed to dental zirconia ceramics in terms of mechanical and physical properties; however, the bonding ability of this material to dental structure and/or veneering ceramics has always been a matter of concern. On the other hand, hydroxyapatite (HA) shows excellent biocompatibility and good bonding ability to tooth structure, with mechanically unstable ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Revista Odonto Ciência

سال: 2018

ISSN: 1980-6523,0102-9460

DOI: 10.15448/1980-6523.2017.4.28749