BACKGROUND AND PURPOSE We previously reported on a randomized controlled trial (RCT) that examined the effect of adding tobramycin to bone cement after femoral stem migration. The present study examined femoral head penetration into both conventional and highly crosslinked polyethylene acetabular liners in the same group of RCT patients, with a minimum of 5 years of postoperative follow-up. P...
متن کاملSequentially Annealed Highly Cross-linked Polyethylene Reduced In Vivo Wear Particle Generation In TKA
Introduction: Polyethylene wear particles induce macrophages to release cytokines, which can lead to osteolysis and aseptic loosening of total joint prostheses. The generation of polyethylene wear particles is one of the most important factors that affect the midterm and long-term clinical results associated with total knee arthroplasty (TKA). Therefore, to achieve better long-term results for ...
متن کاملWear of highly crosslinked polyethylene acetabular components
BACKGROUND AND PURPOSE Wear rates of highly crosslinked polyethylene (XLPE) acetabular components have varied considerably between different published studies. This variation is in part due to the different techniques used to measure wear and to the errors inherent in measuring the relatively low amounts of wear in XLPE bearings. We undertook a scoping review of studies that have examined the i...
متن کاملIn vivo wear of polyethylene acetabular components.
Polyethylene acetabular cups retrieved at revision surgery were measured by a shadowgraph technique to determine linear wear, and the values were compared with those obtained from radiographs. There was a close correlation between them, although the radiographic measurements slightly underestimated the true wear. Average linear wear rates for surface-replacement components were much greater tha...
متن کاملPolyethylene wear from retrieved acetabular cups.
Laboratory wear testing of ultra high molecular weight polyethylene from 12 Charnley acetabular cups, removed after periods of up to 17.5 years showed that the large patient-to-patient variations in clinical penetration rate cannot be explained by batch-to-batch variation in the wear resistance of the material. Nor was there any evidence of a time-dependent degradation in wear resistance of the...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Acta Orthopaedica
سال: 2014
ISSN: 1745-3674,1745-3682
DOI: 10.3109/17453674.2014.949044