The viscoelastic properties of nine silicone-, polysulfide-, and polyether-based impression materials were determined using creep tests. During deformation the materials demonstrated linear viscoelastic behavior. The creep compliance curves, recovery, and percent set were calculated. Permanent deformation in these materials is a result of lack of recovery of elastic deformation as well as visco...

متن کامل

Viscoelastic properties of elastomeric impression materials: polysulphide, silicone and polyether rubbers.

Creep compliance measurements were shown to be effective in characterizing the elastic, retarded elastic, and viscous properties of polysulphide, silicone, and polyether impression materials. The test is particularly valuable in that the creep compliance was independent of load, allowing the mechanical properties to be represented by a single total creep compliance curve which can be used to de...

متن کامل

Antibacterial and antifungal properties of polyether impression materials.

The aim of this study was to evaluate the antibacterial and antifungal properties of polyether impression materials using the agar diffusion test. Three different types of polyether impression materials (P2, Penta Soft and Penta) were tested to determine their ability to inhibit the growth of Enterococcus faecalis, Staphylococcus aureus, Pseudomonas aeruginosa, and Candida albicans. The areas o...

متن کامل

Dynamic viscoelastic properties of experimental silicone soft lining materials.

The purpose of this study was to evaluate the dynamic viscoelastic properties of experimental silicone soft lining materials, Silastic MDX 4-4210 reinforced with silica fillers. Storage modulus (E'), loss modulus (E") and damping factor (tan delta) were determined using a dynamic mechanical analyzer under a deformation strain level of 0.27% at test frequency and a temperature range of 1 Hz and ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of Dental Research

سال: 1974

ISSN: 0022-0345,1544-0591

DOI: 10.1177/00220345740530050301