Variation of Bulk Etch Rate and some other Etching Parameters with Etching Temperature for Cellulose Nitrate LR-115 Detector

نویسندگان

چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Effect of Gamma Rays on The Bulk Etching Rate of LR-115 Detector

It is important to measure the bulk-etching rate for any solid state nuclear track detectors, because they have an application in different fields of sciences. The effect of gamma rays emitted from 60 Co source with different doses on LR-115 detector was studied. The bulk etching rate of the detectors was measured before and after irradiation using gamma source. From the results the values of t...

متن کامل

Measurement of bulk etch rate of LR 115 detector with atomic force microscopy

Equations for calculating track parameters have been proposed, which invariably involve the track etch rate Vt and the bulk etch rate Vb. The present study measured Vb for the LR115 solid-state nuclear track detector using atomic force microscopy (AFM). The detectors were partially masked using rubber cement and then etched in 2:5 N NaOH solution at 60◦C for time periods ranging from 5 to 40 mi...

متن کامل

E ects of stirring on the bulk etch rate of LR 115 detector

The e ects of stirring on the bulk etch rate of LR 115 detector has been investigated. The surface pro6le measurement method using an instrument called Form Talysurf has been used to measure the thickness of the active layer of the LR 115 detectors. The etchant was 10% aqueous solution of NaOH maintained at 60◦C. The bulk etch rate under magnetic stirring has been found to be 6:65 ± 0:34 m h−1 ...

متن کامل

Chemical etching characteristics for cellulose nitrate

Cellulose nitrate films (commercially available as LR 115 films were irradiated systematically with alpha particles in the energy range from 1 to 5 MeV with incident angles from 30◦ to 90◦. After etching to remove a thickness of 6.5 m, the lengths of the major and minor axes of the alpha-particle track openings in the films were measured with an image analyser under an optical magnification of ...

متن کامل

Bulk etch characteristics of colorless LR 115 SSNTD

The colorless LR 115 solid-state nuclear track detector (SSNTD) (from DOSIRAD) is based on cellulose nitrate and was first studied in view of its applicability in radiobiological experiments with alpha particles. In this paper, the bulk etch characteristics were studied. We first showed that the shape of the alpha-particle tracks are irregular with blurred contours under the optical microscope....

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: JOURNAL OF EDUCATION AND SCIENCE

سال: 2009

ISSN: 2664-2530

DOI: 10.33899/edusj.2009.57749