Understanding the High Creep Resistance of MRI 230D Magnesium Alloy through Nanoindentation and Atom Probe Tomography

نویسندگان

چکیده

Due to their low density, magnesium alloys are very appealing for light-weight constructions. However, the use of most common alloy, AZ91 (Mg 9 wt.% Al, 1 Zn), is limited temperatures below 150 °C due creep failure. Several with an improved resistance have been developed in past, example alloy MRI 230D or Ca-alloyed variants. there ongoing discussion literature regarding mechanisms resistance. One factor claimed be responsible intermetallic phases which form during casting. Another possible explanation increased formation precipitates. To gain more insight into 230D, nanoindentation measurements performed on different as-cast, creep-deformed and heat-treated samples These clearly show that phase (IP) does not lose strength deformation contrast High-temperature at 200 maintain strength. This clear variants, where IP significantly softer than room temperature. Atom probe used differences terms chemical composition between IPs variants order understand dissimilar behaviour loss increasing

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Atom probe tomography in nanoelectronics

The role of laser assisted atom probe tomography (APT) in microelectronics is discussed on the basis of various illustrations related to SiGe epitaxial layers, bipolar transistors or MOS nano-devices including gate all around (GAA) devices that were carried out at the Groupe de Physique des Matériaux of Rouen (France). 3D maps as provided by APT reveal the atomic-scale distribution of dopants a...

متن کامل

the relationship between academic self-concept and academic achievement in english and general subjects of the students of high school

according to research, academic self-concept and academic achievement are mutually interdependent. in the present study, the aim was to determine the relationship between the academic self-concept and the academic achievement of students in english as a foreign language and general subjects. the participants were 320 students studying in 4th grade of high school in three cities of noor, nowshah...

Atom Probe Tomography of Oxide Scales

Atom probe tomography, APT, is the only microstructural method that can routinely analyse and position individual atoms in a material with a spatial resolution of 0.1-0.5 nm. Recent implementation of pulsed-laser to APT made investigation of less conducting materials, such as oxides, feasible. In this paper a short description of the principle of the techniques is presented. It is followed by e...

متن کامل

Atom-Probe Tomography of Meteoritic Nanodiamonds

1 Robert A. Pritzker Center for Meteoritics and Polar Studies, The Field Museum of Natural History, Chicago, IL, USA. E-mail: [email protected] 2 Chicago Center for Cosmochemistry, The University of Chicago, Chicago, IL, USA. 3 Northwestern University Center for Atom-Probe Tomography, Department of Materials Science & Engineering, Northwestern University, Evanston, IL, USA. 4 Materials Sci...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Metals

سال: 2021

ISSN: ['2075-4701']

DOI: https://doi.org/10.3390/met11111727