Effect of grinding time on flotation recovery of copper smelting slags in Bardaskan district

Copper smelting slags are hard materials. Therefore,to recover their copper by flotation method, grinding should be carried out to obtain optimal particle size. Copper smelting slags in the Bardeskan district, with work index of 16.24 kwh/st, were grinded for 65 minutes to reach an acceptable degree of freedom for the flotation tests, with particle size of 80%, smaller than 70 μm. With this gri...

متن کامل

IsaMill Ultrafine Grinding for a Sulphide Leach Process

Fine grinding mills have improved in design and efficiency in recent years, allowing major opportunities for treatment of materials where liberation to grind sizes below fifteen microns are required. The successful development of the IsaMill, a horizontal stirred mill, has produced equipment capable of grinding the larger tonnages which exist in mineral processing operations, to product sizes b...

متن کامل

KINETIC STUDIES FOR GOLD LEACHING OF A REFRACTORY SULFIDE CONCENTRATE BY CHLORIDE–HYPOCHLORITE SOLUTION

In this paper, gold leaching of a refractory sulfide concentrate by chloride–hypochlorite solution was investigated and effects of stirring speed, temperature and particle size on the leaching rate were reported. Experimental data for leaching rate of gold were analyzed with the shrinking–core model. Results were consistent with chemical reaction control mechanism in the first 1 h of leachin...

متن کامل

effect of grinding time on flotation recovery of copper smelting slags in bardaskan district

copper smelting slags are hard materials. therefore,to recover their copper by flotation method, grinding should be carried out to obtain optimal particle size. copper smelting slags in the bardeskan district, with work index of 16.24 kwh/st, were grinded for 65 minutes to reach an acceptable degree of freedom for the flotation tests, with particle size of 80%, smaller than 70 μm. with this gri...

متن کامل

Microbial oxidation of refractory gold sulfide concentrate by a native consortium

A defined mesophilic consortium including an iron oxidizing bacterium and a sulfur oxidizing bacterium was constructed to evaluate its ability for bioleaching a flotation concentrate from Andacollo mine in Neuquén, Argentina. Experiments were performed in shake flasks with a pulp density of 10% (w/v), using a basal salt medium containing ferrous iron at pH 1.8. The leaching solutions were analy...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Izvestiya Vuzov Tsvetnaya Metallurgiya (Proceedings of Higher Schools Nonferrous Metallurgy

سال: 2017

ISSN: 2412-8783,0021-3438

DOI: 10.17073/0021-3438-2017-5-13-18