Tool Wear under High Speed End Milling of Nickel-Base Superalloy Inconel 718
نویسندگان
چکیده
منابع مشابه
Investigation of Cutting Forces Superalloy Inconel 718
Since the cutting tools used in machining process of super alloys are subjected to high cutting forces, accordingly tools life is reduced, therefore improvement in alloys machining and reducing cutting forces to achieve longer tools life is an essential necessity. In this research, the effect of changes in feed rate on cutting forces in machining process of nickel based super alloys is investig...
متن کاملCharacterization of strain induced precipitation in Inconel 718 superalloy
Inconel 718 is a Ni-Cr-Fe superalloy which presents excellent mechanical properties at high temperatures, as well as good corrosion resistance and weldability. These characteristics can be optimized with an appropriate control of microstructural features such as grain size and precipitation. Precipitates of different nature can form in these alloys, i.e. γ’’ (a metastable metallic compound Ni3N...
متن کاملEvaluation of Tool Performance With Nanocrystalline Multilayer Coatings on the Machinability of Superalloy Inconel 718
In this paper, the performance of the cutting tool with nanocrystalline multilayer coatings (TiN+TiAlN) for machining of superalloy Inconel 718 in the dry and wet conditions was studied. The multi layer TiN and TiAlN with nanocrystalline structure was applied by physical vapor deposition technique (arc evaporation) on the WC-Co inserts. The results of the ball on disc wear test and the machinin...
متن کاملAn Experimental Study of Tool Wear and Cutting Force Variation in the End Milling of Inconel 718 with Coated Carbide Inserts
ABSTRACT Inconel 718 is a difficult-to-cut nickel-based superalloy commonly used in aerospace industry. This paper presents an experimental study of the tool wear propagation and cutting force variations in the end milling of Inconel 718 with coated carbide inserts. The experimental results showed that significant flank wear was the predominant failure mode affecting the tool life. The tool fla...
متن کاملForce-torque based on-line tool wear estimation system for CNC milling of Inconel 718 using neural networks
In a modern machining system, tool condition monitoring systems are needed to get higher quality production and to prevent the downtime of machine tools due to catastrophic tool failures. Also, in precision machining processes surface quality of the manufactured part can be related to the conditions of the cutting tools. This increases industrial interest for in-process tool condition monitorin...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of the Japan Society for Precision Engineering, Contributed Papers
سال: 2004
ISSN: 1881-8722,1348-8724
DOI: 10.2493/jspe.70.1086