Time-Dependent Crack Growth Thresholds of Ni-Base Superalloys
نویسندگان
چکیده
منابع مشابه
High Temperature Nanoindentation of Ni-base Superalloys
Novel techniques for characterizing and assessing the properties of Ni-base superalloys are becoming increasingly important to the accelerated development of new structural alloys and the advancement of physics-based mechanical property models. Instrumented indentation techniques have long served as a useful approach for probing the mechanical response of a wide range of engineering materials. ...
متن کاملA Thermomechanical Fatigue Crack Initiation Model for Directionally-solidified Ni-base Superalloys
Nickel-base superalloys have been used extensively in power generation applications due to their high strength at temperatures up to 1093°C. When the material is subjected to complex mechanical loading superimposed with thermal loading, fatigue interacts with either creep and/or oxidation. Directionallysolidified (DS) materials are often used in place of polycrystalline (PC) materials since the...
متن کاملCreep Crack Growth Simulation of Ni-base Superalloy
The purpose of this study is to develop a numerical approach to simulate the creep cracking of a Ni-base superalloy. The approach is based in continuum damage mechanics (CDM) and uses the classic Kachanov-Rabotnov constitutive equations for creep deformation and damage evolution. Creep damage takes the form of defects such as microcracks, cavities, voids, etc. A numerical crack growth algorithm...
متن کاملMechanisms of creep deformation in polycrystalline Ni-base disk superalloys
Mechanisms of creep deformation in polycrystalline Ni-base disk superalloys R.R. Unocic a,∗, G.B. Viswanathan a, P.M. Sarosi a, S. Karthikeyan b, J. Li a, M.J. Mills a a Department of Materials Science and Engineering, The Ohio State University, 477 Watts Hall, 2041 College Road, Columbus, OH 43210, USA b Department of Materials Engineering, Indian Institute of Science Bangalore, Karnataka 5600...
متن کاملMicrostructural aspects of fatigue in Ni-base superalloys.
Nickel-base superalloys are primarily used as components in jet engines and land-based turbines. While compositionally complex, they are microstructurally simple, consisting of small (50-1000 nm diameter), ordered, coherent Ni(3)(Al,Ti)-type L1(2) or Ni(3)Nb-type DO(22) precipitates (called γ(') and γ(''), respectively) embedded in an FCC substitutional solid solution consisting primarily of Ni...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Metallurgical and Materials Transactions A
سال: 2014
ISSN: 1073-5623,1543-1940
DOI: 10.1007/s11661-014-2271-8