Thermal fatigue of single-crystal superalloys: experiments, crack-initiation and crack-propagation criteria
نویسندگان
چکیده
منابع مشابه
Thermal activation of fatigue crack growth: analysing the mechanisms of fatigue crack propagation in superalloys
A method for deriving apparent activation energies, Eapp, for fatigue crack growth (FCG) is presented. It is shown how these Eapp values can be used to analyse the main underlying mechanism causing the progression of the crack. The Eapp values for fatigue crack growth in air and vacuum, and with and without a dwell are obtained for a range of Ni based superalloys for turbine disc applications. ...
متن کاملFatigue crack initiation in a notched single-crystal superalloy component
In this paper, the fatigue crack initiation in notched single-crystal test specimens of material MD2 is investigated and analysed. A critical plane approach is adopted, in which the total strain ranges on the discrete slip planes are evaluated. Furthermore, a Coffin-Manson type of expression is used to describe the number of cycles to fatigue crack initiation. This relation is determined from a...
متن کاملEffects of Microstructure on Room Temperature Fatigue Crack Initiation and Short Crack Propagation in Udimet
An assessment of the effects of microstructure on room temperature fatigue crack initiation and short crack propagation in a Ni-base superalloy is presented. The assessment was carried out on microstructural variants of U720Li, including as-received U720Li, U720Li-LG (large grain variant) and U720Li-LP (large intragranular coherent γ′ variant). Fatigue tests were carried out at room temperature...
متن کاملSide Effects of Shot Peening on Fatigue Crack Initiation Life
Shot peening beneficial effects on fatigue life of mechanical components are well known. However, there are some reports in the literature that indicate inappropriate shot peening parameters tend to reduce the fatigue life. It is therefore, the purpose of this study to find a logical quantitative justification for these observations. Using finite element method, a dynamic elastic-plastic simula...
متن کاملEvaluation of Fatigue Crack Initiation in a Notched Single-crystal Superalloy Component
The fatigue crack initiation in a notched single-crystal nickel-base superalloy component at 500°C was investigated and analysed. A critical plane approach in combination with a critical distance method has been adopted, in which the total shear strain ranges on the discrete slip planes are evaluated. Furthermore, a Coffin-Manson type of expression is used to predict the number of cycles to fat...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Materiali in tehnologije
سال: 2015
ISSN: 1580-2949,1580-3414
DOI: 10.17222/mit.2014.251