Liquefied Wood as a Partial Substitute of Melamine-urea- Formaldehyde and Urea-formaldehyde Resins
Maritime pine (Pinus pinaster) sawdust was used to produce liquefied wood by the polyhydric method with acid catalysis. The process was optimized to produce the highest amount of liquefied wood. Wood liquefied at 160oC for 90 min was used in the adhesion tests. The bond strength of veneer glued with ureaformaldehyde and melamine-urea-formaldehyde resins and several mixtures of liquefied wood wi...
متن کاملDevelopment of melamine modified urea formaldehyde resins based on strong acidic pH catalyzed urea formaldehyde polymer
To upgrade the performance of urea-formaldehyde (UF) resin bonded particleboards, melamine modified urea-formaldehyde (MUF) resins based on strong acidic pH catalyzed UF polymers were investigated. The study was conducted in a series of two experiments: 1) formulation of MUF resins based on a UF polymer catalyzed with strong acidic pH and 2) determination of the effects of increased melamine co...
متن کاملUrea-formaldehyde Adhesive Resins*
Approximately 1 million metric tons of urea-formal-dehyde resin are produced annually. More than 70% of this urea-formaldehyde resin is used by the forest products in-*This information was written and prepared by a U.S. Government employee on official time and it is, therefore, in the public domain and not subject to copyright.
متن کاملRattan Cane Modified with Polyethylene Glycol Melamine-Urea-Formaldehyde Resin
To effectively improve the strength of Plectocomia pierreana rattan cane without reducing its toughness, the cane was impregnated with a new water-soluble melamine-urea-formaldehyde (MUF) resin modified with low-molecular-weight polyethylene glycol (PEG), marked as PMUF. The PMUF synthetic process was optimized using an orthogonal test L9(3). Results showed that the dimensional stability, densi...
متن کاملMelamine-modified urea formaldehyde resin for bonding particleboards
For the development of a cost-effective melamine-modified urea formaldehyde resin (MUF), the study evaluated the effects of reaction pH and melamine content on resin properties and bond performance of the MUF resin adhesive systems. Eight resins, each with three replicates, were prepared in a factorial experiment that included two formulation variables: two reaction pHs (i.e., 4.5 and 8.0) and ...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Wood Preservation
سال: 1986
ISSN: 0287-9255,1884-0116
DOI: 10.5990/jwpa.12.4_279