The Thermodynamic Driving Force for Rafting in Superalloys

Eshelby’s energy-momentum tensor is used to provide an analytical expression for the driving force for rafting in the elastic regime in a superalloy with a high volume fraction of 7’. The structure is modelled as a simple cubic array of y’ cubes separated by thin sheets of ;‘. During rafting, the y’ particles are constrained to remain tetragonal prisms. For tension along a cube axis, the drivin...

متن کامل

The driving force for life's emergence: kinetic and thermodynamic considerations.

The principles that govern the emergence of life from non-life remain a subject of intense debate. The evolutionary paradigm built up over the last 50 years, that argues that the evolutionary driving force is the Second Law of Thermodynamics, continues to be promoted by some, while severely criticized by others. If the thermodynamic drive toward ever-increasing entropy is not what drives the ev...

متن کامل

Driving Force for Nucleation of Multi-Component Gas Hydrate

Based on driving force for crystallization of one-component gas hydrate, in this report an expression for the supersaturation for crystallization of multicomponent gas hydrate is derived. Expressions for the supersaturation are obtained in isothermal and isobaric regimes. The results obtained are applied to the crystallization of hydrates of mixtures of methane plus ethane and can apply to ...

متن کامل

the search for the self in becketts theatre: waiting for godot and endgame

this thesis is based upon the works of samuel beckett. one of the greatest writers of contemporary literature. here, i have tried to focus on one of the main themes in becketts works: the search for the real "me" or the real self, which is not only a problem to be solved for beckett man but also for each of us. i have tried to show becketts techniques in approaching this unattainable goal, base...

15 صفحه اول

The thermodynamic driving force for bone growth and remodelling: a hypothesis.

The Eshelby stress (static energy momentum) tensor is derived for bone modelled as an inhomogeneous piezoelectric and piezomagnetic Cosserat (micropolar) medium. The divergence of this tensor is the configurational force felt by material gradients and defects in the medium. Just as in inhomogeneous elastic media, this force is identified with the thermodynamic force for phase transformations, i...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Acta Materialia

سال: 1996

ISSN: 1359-6454

DOI: 10.1016/1359-6454(95)00423-8