چکیده

Nickel-based single crystal superalloy is the most important material for blade preparation. However, some solidification defects inevitably occur during process of preparing single-crystal blades through directional solidification. In this study, in order to study origin misorientation solidification, a model with rejoined platforms was designed according geometry guide vanes. Electron Back-Scattering Diffraction (EBSD) used quantify orientation deviation dendrites and identify platforms. The results showed that stray grain appeared their changed gradually, not abruptly. Combined simulation results, it proposed grains formed as result fragment, which induced by solute enrichment mushy zone Meanwhile, accompanied obvious dendritic deformation, caused shrinkage stress. This suggested fragmentation multiple factors, among which, concave interface shape provided favorable conditions enrichment, dynamic variability local thermal gradient fluctuations rate might play catalytic roles.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

ON THE FORMATION OF STRAY GRAINS IN DIRECTIONALLY-SOLIDIFIED NI-BASED SUPERALLOYS WITH VARYING CROSS SECTIONS

Formation of stray grain defects particularly around re-entrant features of the turbine blade airfoils is one of the major problems in directional and single crystal solidification processes. In this work, directional solidification tests of the GTD-111 Ni-based superalloy were conducted at different withdrawal velocities of 3, 6 and 9 mm.min-1 using various stepped cylindrical and cubic design...

متن کامل

Evaluating the Effect of Ta/W Ratio on Microstructure and Stress Rupture Properties of Ni-Based Single Crystal Superalloy PWA1483

In this study, the effect of Ta/W ratio on the microstructure and stress rupture properties of Ni-based single crystal (SX) superalloy PWA1483 was investigated. For this purpose, single crystal (SX) superalloys with different Ta/W ratios (0.75, 1.0, 1.32 and 1.5 in wt.%) were fabricated. The alloys were directionally solidified by Bridgman method under the same solidification condition at withd...

متن کامل

from linguistics to literature: a linguistic approach to the study of linguistic deviations in the turkish divan of shahriar

chapter i provides an overview of structural linguistics and touches upon the saussurean dichotomies with the final goal of exploring their relevance to the stylistic studies of literature. to provide evidence for the singificance of the study, chapter ii deals with the controversial issue of linguistics and literature, and presents opposing views which, at the same time, have been central to t...

15 صفحه اول

the role of russia in transmission of energy from central asia and caucuses to european union

پس ازفروپاشی شوروی،رشد منابع نفت و گاز، آسیای میانه و قفقاز را در یک بازی ژئوپلتیکی انرژی قرار داده است. با در نظر گرفتن این منابع هیدروکربنی، این منطقه به یک میدانجنگ و رقابت تجاری برای بازی های ژئوپلتیکی قدرت های بزرگ جهانی تبدیل شده است. روسیه منطقه را به عنوان حیات خلوت خود تلقی نموده و علاقمند به حفظ حضورش می باشد تا همانند گذشته گاز طبیعی را به وسیله خط لوله مرکزی دریافت و به عنوان یک واس...

15 صفحه اول

In- and Out-of Phase Thermomechanical Fatigue of a Ni-Based Single-Crystal Superalloy

In this study, the difference between in-phase (IP) and out-of-phase (OP) thermomechanical fatigue (TMF) cycling from 100 to 750 ◦C has been investigated for the Ni-based single-crystal superalloy MD2. In addition, two different crystal orientations were studied, the 〈001〉 and 〈011〉 orientations respectively. When comparing IP and OP TMF lives, a strain range dependency is found for the 〈001〉 d...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Metals

سال: 2023

ISSN: ['2075-4701']

DOI: https://doi.org/10.3390/met13081470