Oxidation behavior of titanium aluminides

Results from an ongoing study of the high temperature oxidation of intermetallic compounds in the Ti-Al system are presented. The oxidation behavior of alloys based on TiAl (y) has been found to be extremely complex depending on temperature and atmosphere composition. Protective alumina scales are formed in pure O2 up to a critical temperature above which a mixed Ti02/A1203 scale forms and grow...

متن کامل

Relation between composition, microstructure and oxidation in iron aluminides

The relation between chemical composition, microstructure and oxidation properties has been investigated on various FeAl based alloys, the aim being to induce changes in the microstructure of the compound by selective oxidation of aluminium. Oxidation kinetics that was evaluated on bulk specimens showed that, due to fast diffusion in the alloys, no composition gradient is formed during the alum...

متن کامل

Incommensurate spin density waves in iron aluminides.

Neutron diffraction in Fe(Al) reveals incommensurate spin density waves (SDWs) in alloys known to be spin glasses. The wave vectors for crystals of Fe(34Al), Fe(40Al), and Fe(43Al) show n varying from 11 to 6 for q-->=2pi(h+/-1/n,k+/-1/n,l+/-1/n)/a(0), where (h,k,l) and a(0) characterize the parent bcc lattice of the CsCl structure. The magnetic reflections are present far above the spin-glass ...

متن کامل

Melting, Casting, and Processing of Nickel and Iron Aluminides Vinod

The nickeland iron-aluminide alloys are an important class of materials because of their unique resistance to oxidizing, carburizing, and sulfidizing environments at high temperatures. They also provide an interesting combination of high-temperature strength and wear resistance. Many applications have been identified for these materials including: furnace fixtures, heating elements, pumps, hydr...

متن کامل

environmental effects of gol-e-gohar iron ore mine on groundwater of the area

gol-e-gohar iron ore mine of sirjan in southern part of iran is a large open pit that operates below the groundwater table and during mining operation, dewatering is required to prevent operation processes from flooding. current operation is going on by digging wells in or out of the pit and pumping to prevent flooding. as a result of the former dewatering operation a vast deep cone of depressi...

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Materials and Corrosion/Werkstoffe und Korrosion

سال: 1996

ISSN: 0947-5117,1521-4176

DOI: 10.1002/maco.19960471202