The present study contains a critical review of work on the formation of precipitates and intermetallic phases in dilute precipitation hardening Al–Cu–Mg based alloys with and without Li additions. Although many suggestions for the existence of pre-precipitates in Al–Cu–Mg alloys with a Cu/Mg atomic ratio close to 1 have been made, a critical review reveals that evidence exists for only two tru...
متن کاملPrecipitation in Powder-metallurgy, Nickel-base Superalloys: Review of Modeling Approach and Formulation of Engineering (postprint)
متن کامل
Residual Stress Assessment in Surface-treated Nickel-base Superalloys
Experimental results are presented to illustrate that there exists a unique window of opportunity for eddy current NDE of residual stress in surface-treated nickel-base superalloys. In light of its frequency-dependent penetration depth, the measurement of eddy current conductivity has been suggested as a possible means to allow the nondestructive evaluation of subsurface residual stresses in su...
متن کاملStrain induced abnormal grain growth in nickel base superalloys
Under certain circumstances abnormal grain growth occurs in Nickel base superalloys during thermomechanical forming. Second phase particles are involved in the phenomenon, since they obviously do not hinder the motion of some boundaries, but the key parameter is here the stored energy difference between adjacent grains. It induces an additional driving force for grain boundary migration that ma...
متن کاملReview on Thermo-Mechanical Fatigue Behavior of Nickel-Base Superalloys
Nickel-base superalloys have become the key materials of hot-end components in the aeroengines over the past several decades. Nickelbase superalloys are easy to produce thermo-mechanical fatigue (TMF) behavior when withstanding the combined effects of high temperature, creep, oxidation, mechanical stress and thermal stress. The occurrence of TMF seriously affects the normal service for hot-end ...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Manufacturing Technology
سال: 2015
ISSN: 1213-2489,1213-2489
DOI: 10.21062/ujep/x.2015/a/1213-2489/mt/15/4/509