Grain Refinement and Enhancement of Mechanical Properties of Hot Extruded Rare-Earth Containing Magnesium Alloy

The effects of rare earth addition and hot extrusion process on the grain refinement of magnesium alloy were studied. The as-cast Mg-6Al-1Zn (AZ61) alloy had the average grain size of ~ 64 µm and its microstructure consisted of α-Mg and Mg17Al12 phase. By partial substitution of Al with Gd to reach Mg-4.8Gd-1.2Al-1Zn alloy, it was observed that the Mg17Al12 phase disappeared and two new interme...

متن کامل

modification of nanoclay for improving the physico-mechanical properties of dental adhesives

هدف اصلی این مطالعه تهیه یک سامانه نوین چسب عاجی دندانی بر پایه نانورس پیوند شده با پلی متاکریلیک اسید، نانورس پیوند شده با پلی اکریلیک اسید، مخلوط نانوسیلیکا و نانورس پیوند شده با پلی متاکریلیک اسید، مخلوط نانوسیلیکا و نانورس پیوند شده با پلی اکریلیک اسید و نانورس پیوند شده با کیتوسان اصلاح شده با گلایسیدیل متاکریلات است. پیوند پلی متاکریلیک اسید و پلی اکریلیک اسید بر ری سطح نانورس در حضور و ...

Microstructure and corrosion characteristics of laser-alloyed magnesium alloy AZ91D with Al-Si powder.

Blown-powder laser surface alloying was performed on the magnesium alloy AZ91D with Al-Si alloy powder to improve corrosion resistance. Characterization by scanning electron microscopy (SEM), energy dispersive spectroscopy (EDS) and x-ray diffraction (XRD) analysis revealed that intermetallic compounds (IMCs) of Mg2Si, Al12Mg17 and Al3Mg2 were formed in the matrix of α-Mg and Al solid solutions...

متن کامل

Microstructure and Aging Behavior of Nonflammable AZ91D Mg Alloy

Phase equilibria of AZ91D Mg alloys for nonflammable use, containing Ca and Y, were carried out by using FactSage® and FTLite database, which revealed that solid solution treatment could be performed at temperatures from 400 to 450C. Solid solution treatment of AZ91D Mg alloy without Ca and Y was successfully conducted at 420C and supersaturated microstructure with all beta phase resolved into ...

متن کامل

Tensile and fatigue behavior of AZ91D magnesium alloy

Recently magnesium alloys, owing to their low density and excellent specific strength have been attractive to designers as an advanced material for coping with energy conservation and environmental pollution regulations. Much of the recent developments of magnesium alloys and processes have been driven by the requirements of the aerospace industry, although some successful ones have found appli...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of Japan Institute of Light Metals

سال: 1995

ISSN: 0451-5994

DOI: 10.2464/jilm.45.391