The Isothermal Oxidation of a New Polycrystalline Turbine Disk Ni-Based Superalloy at 800 °C and Its Modification with Pre-oxidation

نویسندگان

چکیده

Abstract Ni-based superalloys with enhanced oxidation resistance at high temperatures are crucial for next-generation gas turbine engines. A new polycrystalline superalloy (C19) that combines improved microstructural stability environmental has been developed. Its determined through measurements of the specific mass change and morphological evolution formed oxides following furnace exposures 800 °C in air up to 1000 hours; results which were benchmarked against Nimonic 105. C19 showed hybrid Type II/Type III behavior as a marginal Al 2 O 3 former performed similarly established 750 °C. The Wagner model transition from internal external oxide formation predicted should form continuous scale higher temperatures. pre-oxidation treatment 1100 1 hour was, therefore, selected shown dramatically improve during subsequent exposure Oxide cross-sectional analysis protective after treatment, whereas 105 retained discontinuous finger-like intrusions beneath Cr overscale.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Simulation of oxidation-nitridation-induced microstructural degradation in a cracked Ni- based superalloy at high temperature

In turbine engines, high temperature components made of superalloys may crack in a creep process during service. With the inward flux of the gases, e.g. oxygen and nitrogen, along those cracks, the microstructure of the superalloy substrate nearby the cracks may degrade by internal oxidation and nitridation. The aim of this study is to investigate and simulate the oxidation-nitridation-induced ...

متن کامل

extraction and characterization of allium irancum plant extract and its application in the green synthesis of silver nano particles and oxidation of thiocarbony1 compounds

سنتز سبز نانوذرات فلزی (nps) درسالهای اخیر توجه بسیارزیادی را به خود جلب کرده است. زیرا این پروتوکل کم هزینه وسازگار با محیط زیست از روش های استاندارد سنتز. در این پایان نامه ما گزارش میکنیم یک روش ساده و سازگار با محیط زیست برای سنتز نانوذرات نقره با استفاده از محلول آبی عصاره گیاه allium iranicum به عنوان یک عامل کاهش دهنده ی طبیعی. نانو ذرات نقره مشخص شد با استفاده از تکنیک های uv-visible، x...

New Creep-Resistant Cast Alloys with Improved Oxidation Resistance in Water Vapor at 650–800°C

Cast stainless steel CF8C-Plus (19wt%Cr/12%Ni) has excellent creep properties, but limited oxidation resistance above 700°C in environments containing H2O. One strategy to improve the alloy oxidation performance is to increase the Cr and Ni concentration. Two new alloys, with, respectively, 21wt%Cr–15wt%Ni and 22wt%Cr–17.5wt%Ni were therefore developed and their long-term oxidation behaviors in...

متن کامل

Air Plasma Sprayed Bond Coat Oxidation Behavior and its Resistance to Isothermal and Thermal Shock Loading

An experimental investigation was conducted to find the effect of spraying method of coating of Thermal Barrier Coatings (TBCs) on their oxidation behaviour and resistance to various thermal loading. Isothermal and thermal shock tests were performed in order to study oxidation behaviour of air plasma sprayed Bond Coat (BC) and assess its effect on TBCs lifetime under the stated loadings. Specim...

متن کامل

validation of a revised logical-mathematical intelligence scale and exploring its relationship with english language proficiency

نظریه هوش چندگانه قسمتهای متفاوت هوش بشری را مورد بررسی قرار می دهد که با شناخت آن شخص به درک بهتری از توانایی های خود میرسد و در نتیجه سعی در استفاده از آن جهت یادگیری بهتر میکند. همچنین با شناخت استعداد دانش آموزان، فرایند یادگیری بهتر میشود. هدف از انجام دادن این تحقیق بررسی رابطه بین هوش ریاضی و استعداد یادگیری زبان انگلیسی میباشد. برای انجام این تحقیق از پرسشنامه هوش ریاضی که توسط شیرر در ...

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Metallurgical and Materials Transactions

سال: 2022

ISSN: ['1073-5623', '1543-1940']

DOI: https://doi.org/10.1007/s11661-022-06896-8