This work aims to explore WC-G201 high entropy cemented carbides properties fabricated by spark plasma sintering with AlCoCrFeNiTi0.2 and WC as binder phase hard respectively. powder were mixed at the mass ratio of 5: 95, 10: 90 15: 85 respectively, then via SPS 1300℃ for 5min. The results show that has good wettability WC, increase content, hardness alloy decreases gradually, fracture toughness increases first decreases, maximum value is 7.88 MPa m1/2. It estimated comprehensive mechanical property best when content between 5wt% 10wt%.

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

The Effect of sintering temperature on microstructure and hardness of milled WC- 20 wt.% equiatomic (Fe,Co) cemented carbides

In this study, WC–20 wt.% equiatomic (Fe,Co) powder mixture was milled in a planetary ball mill. The effects of different milling time (15 min, 5h, 10h, and 25 h) and sintering temperatures on the microstructure and mechanical properties of this equi-Fe substituted cermet were investigated. The structural evolution and the crystallite size changes of the powders during milling were monitored by...

متن کامل

Effect of WC/Co coherency phase boundaries on Fracture toughness of the nanocrystalline cemented carbides

The effect of coherency WC/Co phase boundaries on the fracture toughness of the nanocrystalline WC-Co cemented carbides is studied by MD simulation method. The simulation results show that the nanocrystalline WC-Co cemented carbides with coherency WC/Co phase boundaries has higher fracture toughness than that without coherency WC/Co phase boundaries. Moreover, the mechanism of why coherency WC/...

متن کامل

Effect of SiC Nanowhisker on the Microstructure and Mechanical Properties of WC-Ni Cemented Carbide Prepared by Spark Plasma Sintering

Ultrafine tungsten carbide-nickel (WC-Ni) cemented carbides with varied fractions of silicon carbide (SiC) nanowhisker (0-3.75 wt.%) were fabricated by spark plasma sintering at 1350°C under a uniaxial pressure of 50 MPa with the assistance of vanadium carbide (VC) and tantalum carbide (TaC) as WC grain growth inhibitors. The effects of SiC nanowhisker on the microstructure and mechanical prope...

متن کامل

Grinding effects on surface integrity and mechanical strength of WC-Co cemented carbides

In this study, the correlation existing among grinding, surface integrity, and flexural strength is investigated for WC-Co cemented carbides (hardmetals). A fine-grained WC-13 wt % Co grade and three different surface conditions: (1) ground, (2) mirror-like polished (reference), and (3) ground plus high-temperature annealed, are investigated. Surface integrity and mechanical characterization is...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Research and application of materials science

سال: 2022

ISSN: ['2661-4456', '2661-4464']

DOI: https://doi.org/10.33142/rams.v4i2.8465