Tensile Fracture Surface Analysis for Boron Fiber.

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Unified tensile fracture criterion.

We find that the classical failure criteria, i.e., maximum normal stress criterion, Tresca criterion, Mohr-Coulomb criterion, and von Mises criterion, cannot satisfactorily explain the tensile fracture behavior of the bulk metallic glass (BMG) materials. For a better description, we propose an ellipse criterion as a new failure criterion to unify the four classical criteria above and apply it t...

متن کامل

Effect on Tensile Strength of Wood-based Carbon Fiber Impregnated by Boron

Wood-based carbon fiber derived from liquefied wood has the disadvantages of low mechanical strength and unstable performance. To improve its mechanical properties, wood-based carbon fiber precursors were impregnated with 5 wt.% and 8 wt.% boric acid solutions for 1 h and then carbonized at 900 °C for 1 h. The effect of boron content on fiber tensile strength and microstructure was investigated...

متن کامل

Electrodeposition of Boron Fiber

From previous experiments, it was determined that nickel was able to coat boron fiber, however this was done unevenly, with cracks characterizing the coating. This was where it was hypothesized that the boron fiber crossed the interface of the nickel electrolyte solution during electrodeposition. This was different than the coating at the middle, which was all under the electrolyte solution, an...

متن کامل

Effects of non-uniform strains on tensile fracture of fiber-reinforced ceramic composites

Effects of non-uniform strains on tensile fracture of fiber-reinforced ceramic–matrix composites have not been satisfactorily explained by existing mechanics-based models. In this paper, we use an exact model of fiber fragmentation under global load sharing conditions to predict fracture in three model problems in which non-uniform strains occur: (i) an end-constrained plate subject to a linear...

متن کامل

Elastic Properties and Fracture Analysis of Perfect and Boron-doped C2N-h2D Using Molecular Dynamics Simulation

   This paper explores the mechanical properties and fracture analysis of C2N-h2D single-layer sheets using classical molecular dynamics (MD) simulations. Simulations are carried out based on the Tersoff potential energy function within Nose-Hoover thermostat algorithm at the constant room temperature in a canonical ensemble. The influences of boron (B) doping on the mechanical properties, ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Journal of the Society of Materials Science, Japan

سال: 1991

ISSN: 1880-7488,0514-5163

DOI: 10.2472/jsms.40.869