Tensile and Creep Testing of Sanicro 25 Using Miniature Specimens

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Tensile and Creep Testing of Sanicro 25 Using Miniature Specimens

Tensile and creep properties of new austenitic steel Sanicro 25 at room temperature and operating temperature 700 °C were investigated by testing on miniature specimens. The results were correlated with testing on conventional specimens. Very good agreement of results was obtained, namely in yield and ultimate strength, as well as short-term creep properties. Although the creep rupture time was...

متن کامل

Tensile Testing of Abalone Nacre Miniature Specimens Using Microscopy and Speckle Correlation

Nacre from seashells, also known as mother-of-pearl, has attracted much attention for its remarkable mechanical properties despite the structural weaknesses of its components [1],[2]. In this article, in situ-tensile tests of dry and wet nacre dogbone specimens are presented. Optical microscopy and digital image correlation techniques were used to determine deformation and strain fields . While...

متن کامل

Creep and Fatigue Interaction Behavior in Sanicro 25 Heat Resistant Austenitic Stainless Steel

Sanicro 25 is a newly developed advanced high strength heat resistant austenitic stainless steel. The material shows good resistance to steam oxidation and flue gas corrosion, and has higher creep rupture strength than other austenitic stainless steels available today. It is thus an excellent candidate for superheaters and reheaters for advanced ultra-super critical power plants with efficiency...

متن کامل

Tensile creep behaviour of polymethylpentenesilica nanocomposites

For the first time, poly(4-methyl-1-pentene) (PMP) nanocomposites were prepared by melt compounding 2 vol% of fumed silica nanoparticles, in order to study the role of the nanofiller surface area and functionalization on the tensile mechanical response of the material, with particular focus on its creep behaviour. The high optical transparency of the polymer matrix was substantially preserved i...

متن کامل

Tensile Creep of Polycrystalline Near-Stoichiometric NiAl

Long term tensile creep studies were conducted on binary NiAl in the temperature range 700-1200 K with the objectives of characterizing and understanding the creep mechanisms. Inverse and normal primary creep curves were observed depending on stress and temperature. It is concluded that the primary creep of NiAl is limited by dislocation mobility. The stress exponent for creep, n, decreased fro...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Materials

سال: 2018

ISSN: 1996-1944

DOI: 10.3390/ma11010142