Tempering and Austempering of Double Soaked Medium Manganese Steels

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

The Silicon Effect in the Tempering of Martensite in Steels

High-silicon steels have long been known to possess exceptional resistance to tempering, but the reasons for this effect were unknown. We report here a study of the third stage of tempering of these steels, in which cementite is formed. In a 0.75 wt% C 1.4 wt% Si alloy steel, tempered for 1 hour at 380°C, it is found that silicon atoms are rejected from the growing cementite into the ferrite ma...

متن کامل

Austenitic Manganese Steels – Developments for Heavy Haul Rail Transportation

In 1882, Sir Thomas Hadfield patented an alloy with quite remarkable properties. Its composition was Fe-1.3%C-13%Mn and it was the toughest alloy known! The claim has stuck for the century since then and the alloy is now used universally for the “frog” in railway crossings in countries such as Canada where heavy loads are moved by rail using high axle loading. In fact, the alloy is very soft wh...

متن کامل

investigating the effect of manganese content on the properties of high manganese austenitic steels

in this study, in order to investigate the effect of increasing the manganese content on microstructure and mechanical properties of high manganese austenitic steels, three alloys with successive increases in weight percentages of manganese (7.55, 13.1, and 16.5) and carbon (0.8 and 1.2) were cast in the presence of a constant amount of chromium (1.5 wt.%) and silica (0.6 wt.%). the samples exp...

متن کامل

Influence of High Strain Rates on the Mechanical Behavior of High-Manganese Steels

In this work, dynamic mechanical properties of three high-manganese steels with TRIP/TWIP or fully TWIP characteristics are studied. High strain rate experiments in the range of true strain rates between ~500 and 1800 /s are conducted using a dynamic torsional testing setup. All the three steels show a positive strain rate sensitivity in the intermediate range of strain rates (up to 500 /s). Bu...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Frontiers in Materials

سال: 2021

ISSN: 2296-8016

DOI: 10.3389/fmats.2020.622131