TEM Study of Precipitation Sequences in Haynes 282 Ni Superalloy
نویسندگان
چکیده
منابع مشابه
Microstructure of Haynes® 282® Superalloy after Vacuum Induction Melting and Investment Casting of Thin-Walled Components
The aim of this work was to characterize the microstructure of the as-cast Haynes® 282® alloy. Observations and analyses were carried out using techniques such as X-ray diffraction (XRD), light microscopy (LM), scanning electron microscopy (SEM), transmission electron microscopy (TEM), X-ray spectroscopy (EDS), wave length dispersive X-ray spectroscopy (WDS), auger electron spectroscopy (AES) a...
متن کاملCreep of Ni-Al and Ni-Cr-Al Superalloy Foams
The steady-state creep rate of Ni-base metallic foams, with superalloy composition (in wt. pct) Ni7.8∼9.1Al (relative density, ρ = 2.5-2.6) and Ni-13.5∼16.6Cr-5.1∼8.9Al (ρ = 2.8∼3.0), was measured under a range of temperatures (680∼825°C) and applied stresses (0.1∼0.3 MPa), and compared with that of NiAl intermetallic foams (ρ = 5.3). The stress exponent and activation energy are within the exp...
متن کاملExamining of Tool Wear in Cryogenic Machining of Cobalt-Based Haynes 25 Superalloy
Haynes 25 alloy (also known as L-605 alloy) is cobalt based super alloy which has widely applications such as aerospace industry, turbine and furnace parts, power generators and heat exchangers and petroleum refining components due to its excellent characteristics. However, the workability of this alloy is more difficult compared to normal steels or even stainless. In present work, an experimen...
متن کاملTemperature Dependence of Residual Stress in Titanium Nitride Coatings on Haynes 188 Superalloy
Residual stresses in TiN coatings deposited by a reactive ion process on Haynes 188 superalloy, for potential application in jet engines, were determined over the temperature range from 30–800 °C, using high temperature X-ray diffraction. In the as-coated condition the TiN films have a pronounced [111] orientation texture and a compressive room temperature stress of -10.5 GPa. After heating for...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Microscopy and Microanalysis
سال: 2018
ISSN: 1431-9276,1435-8115
DOI: 10.1017/s1431927618011480