Tailoring Microstructure and Microsegregation in a Directionally Solidified Ni-Based SX Superalloy by a Weak Transverse Static Magnetic Field

نویسندگان

چکیده

A weak transverse static magnetic field (WTSMF, 0–0.5 T) is applied to the directional solidification process of a DD3 Ni-based SX superalloy, aiming tailor microstructure and microsegregation alloys. The mechanisms microstructural refinement distribution caused by WTSMF during are discussed. It shown that primary dendrite arm spacing rapidly reduced from 181 143 μm, average size γ′ phase significantly refined 0.85 0.25 μm as increases 0 0.5 T. At same time, volume fractions γ/γ′ eutectic segregation coefficient also gradually decreased. 3D numerical simulations multiscale convection in liquid show modifications mainly attributed enhanced flow thermoelectric (TEMC) at dendrite/sample scale under WTSMF. maximum TEMC with increasing intensity. This work paves simple way optimize directionally solidified superalloys without changing processing parameters composition.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Directional Solidification Microstructure of a Ni-Based Superalloy: Influence of a Weak Transverse Magnetic Field

A Ni-based superalloy CMSX-6 was directionally solidified at various drawing speeds (5–20 μm·s−1) and diameters (4 mm, 12 mm) under a 0.5 T weak transverse magnetic field. The results show that the application of a weak transverse magnetic field significantly modified the solidification microstructure. It was found that if the drawing speed was lower than 10 μm·s−1, the magnetic field caused ex...

متن کامل

Effect of a weak transverse magnetic field on the microstructure in directionally solidified peritectic alloys

Effect of a weak transverse magnetic field on the microstructures in directionally solidified Fe-Ni and Pb-Bi peritectic alloys has been investigated experimentally. The results indicate that the magnetic field can induce the formation of banded and island-like structures and refine the primary phase in peritectic alloys. The above results are enhanced with increasing magnetic field. Furthermor...

متن کامل

Thermomechanical Fatigue Behavior of a Directionally Solidified Ni-Base Superalloy

A continuum crystal plasticity model is used to simulate the material behavior of a directionally solidified Ni-base superalloy, DS GTD-111, in the longitudinal and transverse orientations. Isothermal uniaxial fatigue tests with hold times and creep tests are conducted at temperatures ranging from room temperature (RT) to 1038°C to characterize the deformation response. The constitutive model i...

متن کامل

Fatigue-creep-environment Interactions in a Directionally-solidified Ni-base Superalloy

Directionally-solidified (DS) GTD-111 is a Ni-base superalloy designed to withstand damage occurring in the first and second stage blades of gas-powered turbines. Because of the distinctive microstructure of this material, the manner in which fatiguecreep-environment damage mechanisms interact to initiate cracks is sensitive to grain structure and chemical composition. Along with fatigue cyclin...

متن کامل

Simulation of Creep Crack Growth of a Directionally-solidified Ni-base Superalloy

Creep lifetime of turbine blade material subjected to sustained centrifugal forces at elevated temperatures is limited by accumulated inelastic deformation and creep crack growth (CCG). Creep resistance exhibited in conventionally cast polycrystalline (PC) Ni-base superalloy components has been enhanced via solidification techniques. Directional solidification (DS) results in large grain sizes ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Acta Metallurgica Sinica (english Letters)

سال: 2022

ISSN: ['2194-1289', '1006-7191']

DOI: https://doi.org/10.1007/s40195-022-01372-z