Synthesis of highly-uniform titania overcoats on a mesoporous alumina catalyst support by atomic layer deposition and their application in hydroprocessing
نویسندگان
چکیده
The feasibility of gas phase deposition using a Ti alkoxide precursor for precise surface modification catalysts was demonstrated by modifying mesoporous alumina support with oxide overcoat.
منابع مشابه
Synthesis and application of mesoporous gamma alumina granules as iridium catalyst support
Mesoporous gamma-alumina granules, which are known as a common catalyst support in industrial applications were synthesized via the sol gel-oil drop method having a diameter of 1-2 mm. The effect of calcination temperature (450 and 750 °C) on the properties of gamma alumina granules were studied and the functionality of 20 wt% iridium catalyst on the alumina granules for hydrazine decomposition...
متن کاملSynthesis of Pt@TiO2@CNTs Hierarchical Structure Catalyst by Atomic Layer Deposition and Their Photocatalytic and Photoelectrochemical Activity
Pt@TiO2@CNTs hierarchical structures were prepared by first functionalizing carbon nanotubes (CNTs) with nitric acid at 140 °C. Coating of TiO2 particles on the CNTs at 300 °C was then conducted by atomic layer deposition (ALD). After the TiO2@CNTs structure was fabricated, Pt particles were deposited on the TiO2 surface as co-catalyst by plasma-enhanced ALD. The saturated deposition rates of T...
متن کاملLarge-scale synthesis of uniform hexagonal boron nitride films by plasma-enhanced atomic layer deposition
Hexagonal boron nitride (h-BN) has been previously manufactured using mechanical exfoliation and chemical vapor deposition methods, which make the large-scale synthesis of uniform h-BN very challenging. In this study, we produced highly uniform and scalable h-BN films by plasma-enhanced atomic layer deposition, which were characterized by various techniques including atomic force microscopy, tr...
متن کاملHighly stable and reversible lithium storage in SnO2 nanowires surface coated with a uniform hollow shell by atomic layer deposition.
SnO2 nanowires directly grown on flexible substrates can be a good electrode for a lithium ion battery. However, Sn-based (metal Sn or SnO2) anode materials always suffer from poor stability due to a large volume expansion during cycling. In this work, we utilize atomic layer deposition (ALD) to surface engineer SnO2 nanowires, resulting in a new type of hollowed SnO2-in-TiO2 wire-in-tube nanos...
متن کاملSynthesis, characterization, and water oxidation by a molecular chromophore-catalyst assembly prepared by atomic layer deposition. The “mummy” strategy
A new strategy for preparing spatially-controlled, multi-component films consisting of molecular light absorbing chromophores and water oxidation catalysts on high surface area, mesoporous metal oxide surfaces is described. Atomic layer deposition (ALD) is used to embed a surface-bound chromophore in a thin layer of inert Al2O3, followed by catalyst binding to the new oxide surface. In a final ...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Catalysis Science & Technology
سال: 2023
ISSN: ['2044-4761', '2044-4753']
DOI: https://doi.org/10.1039/d3cy00335c