Study of Tantalum Substituted Potassium Tungsten Bronzes
نویسندگان
چکیده
منابع مشابه
Bridging the opposite chemistries of tantalum and tungsten polyoxometalates.
The disparate solubility, redox activity, and pH stability of the group V and group VI polyoxometalates (POMs) confer very different functionality on these species, and tailoring cluster properties by varying the ratio of group V to group VI metals poses both an opportunity and a synthetic challenge. A classic series of studies reported over 40 years ago provided some insight into W/Nb POMs, fr...
متن کاملHysteresis and memory effects in irradiated potassium blue bronzes
2014 Molybdenum blue bronzes exhibit below the Peierls transition time-dependent phenomena. These properties, which are related to the charge density wave instability, are often associated to the presence of defects. In this paper we show that the hysteresis observed during temperature cycling is amplified when defects are introduced by irradiation. We describe two new phenomena observed after ...
متن کاملTowards novel multiferroic and magnetoelectric materials: dipole stability in tetragonal tungsten bronzes.
We discuss the strategy for development of novel functional materials with the tetragonal tungsten bronze structure. From the starting composition Ba6GaNb9O30, the effect of A- and B-site substitutions on the dielectric properties is used to develop an understanding of the origin and stability of the dipolar response in these compounds. Both tetragonal strain induced by large B-site cations and...
متن کاملPhosphine-Substituted Diborane(4)yl Complexes of Tungsten
The reaction of the 1,2-dihalodiborane(4) B2(NMe2)2Cl2 with the lithium tungsten salts Li[(η5C5H5)(R3P)(OC)2W] [R = Me (3a), Ph (3b)] yields via alkali salt elimination the phosphinesubstituted diborane(4)yl tungsten complexes [(η-C5H5)(R3P)(OC)2W-{B(NMe2)-B(NMe2)Cl}] [R = Me (4a), Ph (4b)]. Both compounds have been fully characterized in solution by NMR and IR spectroscopy and 4a additionally ...
متن کاملThe influence of tungsten alloying on the mechanical properties of tantalum
In mechanical tests of tantalum-tungsten alloys with nominal tungsten contents between 0 and 10 wt% for strain rates between 0.000016 and 6800 sr and temperatures between 77 and 400 K, the addition of tungsten noticeably reduces the strain-rate dependence of the flow stress of tantalum near yield. It also subtly alters the strain-rate behavior of the work hardening, making it more like that of ...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of the Bangladesh Chemical Society
سال: 2012
ISSN: 2408-8692,1022-016X
DOI: 10.3329/jbcs.v25i1.11770