Study of Anodic Film’s Surface and Hardness on A356 Aluminum Alloys, Using Scanning Electron Microscope and In-Situ Nanoindentation

نویسندگان

چکیده

The A356 aluminum alloy is a very commonly used in the automotive industry, for parts such as pistons, cylinder heads, and connecting rods, which mechanical properties can be effectively increased by anodizing. In this work, oxide layers were formed oxalic acid solution with defined parameters on then studied using novel combination of scanning electron microscope (SEM) in-situ nanoindentation. purpose research to understand relationship between substrate layer examining its microstructure nanohardness. Based experimental results showing special composite corresponding high hardness, seems good alternative replacing steel brake disks an environmentally conscious manner.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

the study of bright and surface discrete cavity solitons dynamics in saturable nonlinear media

امروزه سالیتون ها بعنوان امواج جایگزیده ای که تحت شرایط خاص بدون تغییر شکل در محیط منتشر می-شوند، زمینه مطالعات گسترده ای در حوزه اپتیک غیرخطی هستند. در این راستا توجه به پدیده پراش گسسته، که بعنوان عامل پهن شدگی باریکه نوری در آرایه ای از موجبرهای جفت شده، ظاهر می گردد، ضروری است، زیرا سالیتون های گسسته از خنثی شدن پراش گسسته در این سیستم ها بوسیله عوامل غیرخطی بوجود می آیند. گسستگی سیستم عامل...

preparation and characterization of new co-fe and fe-mn nano catalysts using resol phenolic resin and response surface methodology study for fischer-tropsch synthesis

کاتالیزورهای co-fe-resol/sio2و fe-mn-resol/sio2 با استفاده از روش ساده و ارزان قیمت همرسوبی تهیه شدند. از رزین پلیمری resol در فرآیند تهیه کاتالیزور استفاده شد.

surface treatment by different parameters of erbium:yttrium–aluminum–garnet (er:yag) laser: scanning electron microscope (sem) evaluation

introduction: this study aimed to assess the scanning electron microscope (sem) analysis of tooth surface irradiated by erbium:yttrium–aluminum–garnet (er:yag) laser with various parameters. methods: number of 25 extracted human third molars free of caries were used in this study. the teeth were put into 5 groups for laser irradiation as follows: group 1 (power: 0.5 w, energy: 50 mj); group 2 (...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Coatings

سال: 2022

ISSN: ['2079-6412']

DOI: https://doi.org/10.3390/coatings12101528