Structural Properties of Mechanically Activated Rare-Earth Manganites
نویسندگان
چکیده
منابع مشابه
Dynamic and structural properties of orthorhombic rare-earth manganites under high pressure
D. A. Mota,1 A. Almeida,1 V. H. Rodrigues,2 M. M. R. Costa,2 P. Tavares,3 P. Bouvier,4 M. Guennou,5 J. Kreisel,5,6 and J. Agostinho Moreira1,* 1Instituto de Fı́sica dos Materiais da Universidade do Porto and Institute of Nanoscience and Nanotechnology, Departamento de Fı́sica e Astronomia da Faculdade de Ciências, Universidade do Porto, Rua do Campo Alegre, 687, 4169-007 Porto, Portugal 2Centro d...
متن کاملMagnetic Phases of Rare Earth Hexagonal Manganites
We describe the magnetic phases of hexagonal rare earth manganites RMnO3 using Landau theory. A minimal model based on four one-dimensional magnetic order parameters is developed.
متن کاملLow-energy structural dynamics of ferroelectric domain walls in hexagonal rare-earth manganites
Domain walls (DWs) in ferroic materials, across which the order parameter abruptly changes its orientation, can host emergent properties that are absent in the bulk domains. Using a broadband (106 to 1010 Hz) scanning impedance microscope, we show that the electrical response of the interlocked antiphase boundaries and ferroelectric DWs in hexagonal rare-earth manganites (h-RMnO3) is dominated ...
متن کاملField Dependent Specific-Heat of Rare Earth Manganites
The low temperature specific heat C(H) of several rare-earth manganites (La0.7Sr0.3MnO3, Nd0.5Sr0.5MnO3, Pr0.5Sr0.5MnO3, La0.67Ca0.33MnO3, La0.5Ca0.5MnO3, La0.45Ca0.55MnO3 and La0.33Ca0.67MnO3) was measured as a function of magnetic field. We observed behaviour consistent with thermodynamic expectations, i.e., C(H) decreases with field for ferromagnetic metallic compounds by an amount which is ...
متن کاملStructural and Thermoelectric Properties of Rare-Earth-Substituted Sr3Fe2O7
The structural and thermoelectric properties of rare-earth (Sm)-substituted RuddlesdenPopper-type Sr3Fe2O7, Sr31xSmxFe2O7 (SSFO, x = 0, 0.1, 0.15), were investigated by measuring the temperature dependence of its crystallographic parameters, electrical conductivity, and Seebeck coefficient (S). A sharp increase in electrical conductivity (·) up to 60 S/cm (log · = 1.78 S/cm) at 400500°C occur...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Chemical and Materials Engineering
سال: 2014
ISSN: 2332-1032,2332-1067