Strong etching formulation (time and rate) for PADC with deep depth bulk etch rate study

نویسندگان

چکیده

Aqueous NaOH with ethanol (strong) etchant is widely used. It shortens etching time effectively compared to normal conditions (6.25N at 70 °C). Two equations have been proposed calculate the molarity and volume. Another two empirical were introduced for estimating bulk etch rates of PADC etched in strong etchant. Up now, there no such available literature that can predict V b volumes. The fundamental models stemming from literature. Fast enables follow-up rate variation versus depth detector material up ? 80 ? m. In agreement previous studies, an equation given which allows variations be expressed under form a reciprocal normalized (i.e., removed layer). • Bulk CR-39 NaOH/ethanol are presented. Advantages NaOH+ethanol against standard aqueous solutions considered. New as function volume given. corresponding illustrated.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

An optimal policy for deteriorating items with time-proportional deterioration rate and constant and time-dependent linear demand rate

In this paper, an economic order quantity (EOQ) inventory model for a deteriorating item is developed with the following characteristics: (i) The demand rate is deterministic and two-staged, i.e., it is constant in first part of the cycle and linear function of time in the second part. (ii) Deterioration rate is time-proportional. (iii) Shortages are not allowed to occur. The o...

متن کامل

a study on rate making and required reserves determination in reinsurance market: a simulation

reinsurance is widely recognized as an important instrument in the capital management of an insurance company as well as its risk management tool. this thesis is intended to determine premium rates for different types of reinsurance policies. also, given the fact that the reinsurance coverage of every company depends upon its reserves, so different types of reserves and the method of their calc...

Measurement of bulk etch rate of LR 115 detector with atomic force microscopy

Equations for calculating track parameters have been proposed, which invariably involve the track etch rate Vt and the bulk etch rate Vb. The present study measured Vb for the LR115 solid-state nuclear track detector using atomic force microscopy (AFM). The detectors were partially masked using rubber cement and then etched in 2:5 N NaOH solution at 60◦C for time periods ranging from 5 to 40 mi...

متن کامل

The form of etch rate minima in wet chemical anisotropic etching of silicon

Etching of monocrystalline silicon in alkaline based solutions leads to a deep minimum in the etch rate crystallographically oriented along 〈111〉. The details of the form of the minimum (angular dependence of the etch rate) are investigated and discussed in a framework of steps originating from spontaneous nucleation and from misorientation of the crystal face exposed to the etchant. As a resul...

متن کامل

Bulk Etch Rate Measurements and Calibrations of Plastic Nuclear Track Detectors

New calibrations of CR39 and Makrofol nuclear track detectors have been obtained using 158 A GeV Pb and In ions; a new method for the bulk etch rate determination, using both cone height and base diameter measurements was developed. The CR39 charge resolution based on the etch-pit base area measurement is adequate to identify nuclear fragments in the interval 7 ≤ Z/β ≤ 49. For CR39 the detectio...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Nuclear Instruments and Methods in Physics Research

سال: 2021

ISSN: ['1872-9576', '0168-9002']

DOI: https://doi.org/10.1016/j.nima.2021.165402