Stress rupture properties of GH4169 superalloy
                    
                        
                            نویسندگان
                            
                            
                        
                        
                    
                    
                    چکیده
منابع مشابه
Evaluating the Effect of Ta/W Ratio on Microstructure and Stress Rupture Properties of Ni-Based Single Crystal Superalloy PWA1483
In this study, the effect of Ta/W ratio on the microstructure and stress rupture properties of Ni-based single crystal (SX) superalloy PWA1483 was investigated. For this purpose, single crystal (SX) superalloys with different Ta/W ratios (0.75, 1.0, 1.32 and 1.5 in wt.%) were fabricated. The alloys were directionally solidified by Bridgman method under the same solidification condition at withd...
متن کاملInvestigation into Grindability of Gh4169 Superalloy and Effects of Grinding Parameters on the Surface Integrity
GH4169, a nickel-base heat-resistant alloy, usually has outstanding high-temperature strength, excellent thermal stability and good wear resistance. However, it is hard to cut and its machined surface quality and integrity are particularly sensitive to a manufacturing process employed. The study reported in this paper was conducted to initially, review existing research on machining-induced sur...
متن کاملcontrol of the optical properties of nanoparticles by laser fields
در این پایان نامه، درهمتنیدگی بین یک سیستم نقطه کوانتومی دوگانه(مولکول نقطه کوانتومی) و میدان مورد مطالعه قرار گرفته است. از آنتروپی ون نیومن به عنوان ابزاری برای بررسی درهمتنیدگی بین اتم و میدان استفاده شده و تاثیر پارامترهای مختلف، نظیر تونل زنی(که توسط تغییر ولتاژ ایجاد می شود)، شدت میدان و نسبت دو گسیل خودبخودی بر رفتار درجه درهمتنیدگی سیستم بررسی شده اشت.با تغییر هر یک از این پارامترها، در...
15 صفحه اولA new dental superalloy system. II. Mechanical properties.
Theoretical considerations that lead to the design of strong and ductile cobalt (Co)base alloys were discussed in part I of this series of articles.' It was hypothesized that the composition 40 Co-30 nickel (Ni)-30 chromium (Cr) is an acceptable compromise for the requirements of an alloy base. It also was found that tantalum (Ta) may have the qualities that are acceptable for an additional ele...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of Materials Research and Technology
سال: 2014
ISSN: 2238-7854
DOI: 10.1016/j.jmrt.2014.03.003