Stress-Rupture Characterization in Nickel-Based Superalloy Gas Turbine Engine Components
نویسندگان
چکیده
منابع مشابه
Gas-Dynamic Modeling of Gas Turbine Engine Components Collaborative Workflow
The aim of this article was the development of the gas-dynamic models allowing to calculate the working processes of the gas turbine engine (GTE) in the compressor, in the combustion chamber and in the turbine at the same time. The possibilities of software systems for complex engine workflow modeling are specified. The advantages and disadvantages of the presented methods are specified. The re...
متن کاملCAPABILITY OF 718Plus FOR STRUCTURAL GAS TURBINE ENGINE COMPONENTS (PREPRINT)
Recent developments from the cast 718Plus® Metals Affordability Initiative (MAI) program will be presented and discussed. The objective of the program is to investigate and enable the use of 718Plus® (hereinafter referred to as 718Plus) in the form of investment castings by (1) increasing the allowable operating temperature by about 75°F as compared with conventional cast Alloy 718 and (2) achi...
متن کاملGas Turbine Engine Behavioral Modeling
This paper develops and validates a power flow behavioral model of a gas turbine engine with a gas generator and free power turbine. “Simple” mathematical expressions to describe the engine’s power flow are derived from an understanding of basic thermodynamic and mechanical interactions taking place within the engine. The engine behavioral model presented is suitable for developing a supervisor...
متن کاملA Silicon-Based Micro Gas Turbine Engine for Power Generation
This paper reports on our research in developing a micro power generation system based on gas turbine engine and piezoelectric converter. The micro gas turbine engine consists of a micro combustor, a turbine and a centrifugal compressor. Comprehensive simulation has been implemented to optimal the component design. We have successfully demonstrated a silicon-based micro combustor, which consist...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of Failure Analysis and Prevention
سال: 2008
ISSN: 1547-7029,1864-1245
DOI: 10.1007/s11668-008-9168-z