Stress corrosion cracking and fracture behaviors of gaseous-hydrogenated Titanium alloy Ti-6321 during slow strain rate tests
نویسندگان
چکیده
منابع مشابه
Assessment of Stress Corrosion Cracking on Pipeline Steels Weldments Used in the Petroleum Industry by Slow Strain Rate Tests
متن کامل
Acoustic Emission during Stress Corrosion Cracking Test
AE monitoring from various types of stress corrosion cracking (SCC) has been conducted for the past 15 years in our laboratory. This paper discusses AE results of active-path dissolution-type SCC of austenitic stainless steel in chloride solution and fused salt, fluoride and polythionic acid solutions, brass in ammonia (Mattosson's solution), and carbon steels in nitrite solution. Transgranular...
متن کاملEffect of Hydrogen on Corrosion and Stress Corrosion Cracking of AZ91 Alloy in Aqueous Solutions
The effect of hydrogen on the corrosion and stress corrosion cracking of the magnesium AZ91 alloy has been investigated in aqueous solutions. Hydrogen produced by corrosion in water diffuses into, and reacts with the Mg matrix to form hydride. Some of the hydrogen accumulates at hydride/Mg matrix (or secondary phase) interfaces as a consequence of slow hydride formation and the incompatibility ...
متن کاملFatigue and corrosion fatigue properties of Ti-6Al-4V implant grade titanium alloy in Ringer solution
Nowadays modification of metallic biomaterials which are used as implants for bone and hard tissues replacement is considered as an important subject. In the current study, corrosion fatigue properties of Ti-6Al-4V alloy investigated via Rotating-Bending standard test method and then, the results compared with the fatigue properties of the specimens tested in the same conditions. Scanning elect...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Materials Research Express
سال: 2021
ISSN: 2053-1591
DOI: 10.1088/2053-1591/abf8e7