Strengthening of Reinforced Concrete Slab-Column Connections with Carbon Fiber Reinforced Polymer Laminates

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Strengthening of Corrosion-Damaged Reinforced Concrete Beams with Glass Fiber Reinforced Polymer Laminates

Problem statement: This study showed the results of an experimental investigation on the strengthening of corrosion damaged reinforced concrete beams with unidirectional cloth glass fiber reinforced polymer (UDCGFRP) laminates. Approach: All the beam specimens 150×250×3000 mm were cast and tested for the present investigation. One beam specimen was neither corroded nor strengthened to serve as ...

متن کامل

Finite Element Modeling of GFRP-Reinforced Concrete Interior Slab-Column Connections Subjected to Moment Transfer

A finite element model (FEM) was constructed using specialized three-dimensional (3D) software to investigate the punching shear behavior of interior slab-column connections subjected to a moment-to-shear ratio of 0.15 m. The FEM was then verified against the experimental results of full-scale interior slab-column connections reinforced with glass fiber reinforcement polymer (GFRP) bars previou...

متن کامل

Flexural Cracks in Fiber-Reinforced Concrete Beams with Fiber-Reinforced Polymer Reinforcing Bars

Fiber-reinforced polymer (FRP) reinforcing bars have aTtracted considerable 0llellli0l1 for applications where corrosion of steel reinforcement is problemaric. Due 10 rhe generally low elastic modulus and poor bond clwracreristics of FRP as coil/pared 10 steel reinforcing bars, the use of FRP results in IGI:i?er crack widlhs under senJice loads. Fiber-reinforced concrete (FRe) is proposed for u...

متن کامل

Strengthening reinforced concrete T connections by steel straps

The aim of this paper is to present results of testing a full scale reinforced concrete T connection by static loading. The connection is a T connection representing a beam-column connection. The beam and column had a square cross section with a 300 mm dimension. The height of the column was 2.9 m and the clear beam length was 1.4 m. The connection was initially tested to failure. Galvanised st...

متن کامل

Subtitle Micro - Macro Modeling of the External Strengthening of Concrete with Fiber Reinforced Polymer : Phase I

A large number of bridges in the federal inventory are reaching the end of their design life due to aging and environmental degradation. The situation is aggravated by increased traffic needs that require existing structures to carry heavier loads at increasingly higher speeds. Project Summary: The issue of moisture diffusion in composite materials is important because of its associated problem...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Applied Sciences

سال: 2019

ISSN: 2076-3417

DOI: 10.3390/app10010265