Speed Up of Steel Rolling and Forming

نویسندگان

چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Hot Forming of Aisi A2 Tool Steel

In order to optimize the hot forming process of tool steels, further improvement of flow stress prediction and additional knowledge on hot deformability, especially at lower and upper limits of the hot working range, are required. The hot working ranges for these steels are very narrow as a consequence of the role of alloying elements, which form carbides. Carbides improve tool steel’s hardenab...

متن کامل

Cold End Forming Of Welded Steel Tubes

The production of custom and specific tube end shapes by cold end forming using a die is generally limited to seamless tubular parts. Current research work in the field follows the same trend as that of industry and, therefore, there is no accumulated experience, no practical design rules, and no information available in the specialized literature concerning the utilization of tube end forming ...

متن کامل

Influence of Rolling on Microstructure and Mechanical Properties of Bronze-Steel Explosive Welded Sheets

In this paper, the microstructure and mechanical properties of the plain carbon steel-bronze interface of explosive welding and rolling were investigated. Explosive connection was done at two stop distances and with two different thicknesses of explosive material. Rolling of the welded composite was done at both ambient and preheated temperatures of 300 °C and with a constant thickness reductio...

متن کامل

Influence of Rolling on Microstructure and Mechanical Properties of Bronze-Steel Explosive Welded Sheets

In this paper, the microstructure and mechanical properties of the plain carbon steel-bronze interface of explosive welding and rolling were investigated. Explosive connection was done at two stop distances and with two different thicknesses of explosive material. Rolling of the welded composite was done at both ambient and preheated temperatures of 300 °C and with a constant thickness reductio...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Tetsu-to-Hagane

سال: 1990

ISSN: 0021-1575,1883-2954

DOI: 10.2355/tetsutohagane1955.76.12_2065