Shearing of γ′ precipitates in Ni-base superalloys: a phase field study incorporating the effective γ-surface

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Modeling displacive–diffusional coupled dislocation shearing of c0 precipitates in Ni-base superalloys

In Ni-base superalloys, superlattice extrinsic stacking fault (SESF) shearing of c0 precipitates involves coupled dislocation glide and atomic diffusion. A phase-field model is developed to study this process, in which the free energy of the system is formulated as a function of both displacement and long-range order parameter. The free energy surface is fitted to various fault energy data obta...

متن کامل

Interdiffusion Behavior of Pt-Diffused γ+γ' Coatings on Ni-Based Superalloys

Platinum-diffused γ+γ' coatings (~20 at.% Al, ~22 at.% Pt) were synthesized on René 142 and René N5 Ni-based superalloys by electroplating the substrates with ~7 μm of Pt, followed by an annealing treatment in vacuum at 1175°C. In order to study the compositional and microstructural evolution of these coatings at elevated temperatures, interdiffusion experiments were carried out on coated speci...

متن کامل

Automated Identification and Characterization of Secondary & Tertiary Γ’ Precipitates in Nickel-based Superalloys (preprint)

The public reporting burden for this collection of information is estimated to average 1 hour per response, including the time for reviewing instructions, searching existing data sources, gathering and maintaining the data needed, and completing and reviewing the collection of information. Send comments regarding this burden estimate or any other aspect of this collection of information, includ...

متن کامل

High Temperature Nanoindentation of Ni-base Superalloys

Novel techniques for characterizing and assessing the properties of Ni-base superalloys are becoming increasingly important to the accelerated development of new structural alloys and the advancement of physics-based mechanical property models. Instrumented indentation techniques have long served as a useful approach for probing the mechanical response of a wide range of engineering materials. ...

متن کامل

Flow Stress Modeling in a γ-γ/ Cobalt Base Superalloy by Using the Hyperbolic Sine Equation and ANN Method

The new class of wrought γ-γ/ Co-base superalloys, which are based on Co-Al-W system,  was developed by conventional hot working routes with a high volume fraction of γ/ precipitates and good mechanical properties. The aim of the present study was to predict the flow stress and hot deformation modeling of a novel γ-γ/ Co-base superalloy. The hot compression test...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Philosophical Magazine

سال: 2012

ISSN: 1478-6435,1478-6443

DOI: 10.1080/14786435.2011.630691