Secondary electron emissive thin film fabricated by atomic layer deposition
نویسندگان
چکیده
منابع مشابه
Bi-layer Channel AZO/ZnO Thin Film Transistors Fabricated by Atomic Layer Deposition Technique
This letter demonstrates bi-layer channel Al-doped ZnO/ZnO thin film transistors (AZO/ZnO TFTs) via atomic layer deposition process at a relatively low temperature. The effects of annealing in oxygen atmosphere at different temperatures have also been investigated. The ALD bi-layer channel AZO/ZnO TFTs annealed in dry O2 at 300 °C exhibit a low leakage current of 2.5 × 10-13A, I on/I off ratio ...
متن کاملThermo-Optical Properties of Thin-Film TiO2–Al2O3 Bilayers Fabricated by Atomic Layer Deposition
We investigate the optical and thermo-optical properties of amorphous TiO2–Al2O3 thin-film bilayers fabricated by atomic layer deposition (ALD). Seven samples of TiO2–Al2O3 bilayers are fabricated by growing Al2O3 films of different thicknesses on the surface of TiO2 films of constant thickness (100 nm). Temperature-induced changes in the optical refractive indices of these thin-film bilayers a...
متن کاملAtomic layer deposition (ALD): from precursors to thin film structures
The principles of the atomic layer deposition (ALD) method are presented emphasizing the importance of precursor and surface chemistry. With a proper adjustment of the experimental conditions, i.e. temperatures and pulsing times, the growth proceeds via saturative steps. Selected recent ALD processes developed for films used in microelectronics are described as examples. These include depositio...
متن کاملThin, high atomic weight refractory film deposition for diffusion barrier, adhesion layer, and seed layer applications
Related Articles The Si3N4/TiN Interface: 4. Si3N4/TiN(001) Grown with a −250 V Substrate Bias and Analyzed In situ using Angle-resolved X-ray Photoelectron Spectroscopy Surf. Sci. Spectra 19, 62 (2012) The Si3N4/TiN Interface: 1. TiN(001) Grown and Analyzed In situ using Angle-resolved X-ray Photoelectron Spectroscopy Surf. Sci. Spectra 19, 33 (2012) The Si3N4/TiN Interface: 5. TiN/Si3N4 Grown...
متن کاملZnS-based photonic crystal phosphors fabricated using atomic layer deposition
The infiltration by atomic layer deposition of three-dimensional opal structures has been investigated as a means of fabricating photonic crystal phosphors. ZnS:Mn infiltrated and inverse opals have been demonstrated with filling fractions >95%. Characterization of these structures by scanning electron microscopy, specular reflectance, and photoluminescence is reported. Specular reflectance mea...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: IOP Conference Series: Materials Science and Engineering
سال: 2019
ISSN: 1757-899X
DOI: 10.1088/1757-899x/612/3/032103