Scratch hardness of rare-earth substituted calcium aluminosilicate glasses
نویسندگان
چکیده
منابع مشابه
Structure of Rare-Earth Aluminosilicate Glasses Probed by Solid-State NMR Spectroscopy and Quantum Chemical Calculations
Results presented in this thesis are based on the following publications, which are referred to by the corresponding roman numbers I-IV: Reprints were made with the permission from the publishers.
متن کاملYb-Sensitized Rare-Earth Doped Optical Glasses
The temperature e ect upon infrared-to-visible frequency upconversion uorescence emission in o -resonance infrared excited Yb-sensitized rare-earth doped optical glasses is theoretically and experimentally investigated. We have examined samples of Er3+/Yb-codoped Ga2S3:La2O3 chalcogenide glasses and germanosilicate optical bers, and Ga2O3:La2O3 chalcogenide and uoroindate glasses codoped with P...
متن کاملCATION UPTAKE PROPERTIES OF CALCIUM ALUMINOSILICATE
In this study, the effect of different parameters such as time and temperature of calcination and milling on the formation of calcium aluminosilicates was investigated. Raw materials used in this study were calcium carbonate and kaolin in high purity. Powder X-ray diffraction patterns were obtained from all samples after heat treatment at various temperatures and times. To study the microstruct...
متن کاملAtomic Structure of Rare Earth Si-Al-O-N Glasses
In this paper the results of X-ray diffraction experiments of Ln-Si-Al-O-N (Ln = La, Gd, Yb) glasses are presented. Total structure factors and pair correlation functions allow the determination of the first coordination sphere of Ln atoms. The bond lengths observed correspond to the ionic radii of the Ln-ions surrounded by oxygen and nitrogen atoms. The presence of non-bridging nitrogen is dis...
متن کاملStructural and Thermoelectric Properties of Rare-Earth-Substituted Sr3Fe2O7
The structural and thermoelectric properties of rare-earth (Sm)-substituted RuddlesdenPopper-type Sr3Fe2O7, Sr31xSmxFe2O7 (SSFO, x = 0, 0.1, 0.15), were investigated by measuring the temperature dependence of its crystallographic parameters, electrical conductivity, and Seebeck coefficient (S). A sharp increase in electrical conductivity (·) up to 60 S/cm (log · = 1.78 S/cm) at 400500°C occur...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Journal of Non-Crystalline Solids: X
سال: 2019
ISSN: 2590-1591
DOI: 10.1016/j.nocx.2019.100010