Robust nanoporous alumina monoliths by atomic layer deposition on low-density carbon-nanotube scaffolds
نویسندگان
چکیده
منابع مشابه
Varying Phases of Alumina Nanowires Templated by Vertically Aligned Carbon Nanotubes Grown via Atomic Layer Deposition
Typically, alumina nanowires (NWs) are synthesized via physical evaporation, templated anodized aluminum oxide (AAO), or the vapor-liquid-solid (VLS) process [1,2,3]. All of these techniques have been shown to demonstrate successful growth of alumina NWs; however, in the cases where a facile method resulting in vertically aligned NWs is desired, many of these methods are difficult to integrate ...
متن کاملSub-5 nm nanostructures fabricated by atomic layer deposition using a carbon nanotube template.
The fabrication of nanostructures having diameters of sub-5 nm is very a important issue for bottom-up nanofabrication of nanoscale devices. In this work, we report a highly controllable method to create sub-5 nm nano-trenches and nanowires by combining area-selective atomic layer deposition (ALD) with single-walled carbon nanotubes (SWNTs) as templates. Alumina nano-trenches having a depth of ...
متن کاملMultiscale Simulation of Atomic Layer Deposition in a Nanoporous Material
A multiscale simulator for alumina film growth inside a nanoporous material during an atomic layer deposition process is developed. The model combines a continuum description at the macroscopic level of precursor gas transport inside a nanopore during exposure to each of the two precursor species (trimethyaluminum and water) with a lattice Monte Carlo simulation of the film growth on the micros...
متن کاملRobust, functional nanocrystal solids by infilling with atomic layer deposition.
Thin films of colloidal semiconductor nanocrystals (NCs) are inherently metatstable materials prone to oxidative and photothermal degradation driven by their large surface-to-volume ratios and high surface energies. (1) The fabrication of practical electronic devices based on NC solids hinges on preventing oxidation, surface diffusion, ripening, sintering, and other unwanted physicochemical cha...
متن کاملPorous Alumina Protective Coatings on Palladium Nanoparticles by Self-Poisoned Atomic Layer Deposition
Atomic layer deposition (ALD) of Al2O3 using trimethylaluminum (TMA) and water on Pd nanoparticles (NPs) was studied by combining in situ quartz crystal microbalance (QCM) measurements, in situ quadrupole mass spectrometry (QMS), and transmission electron microscopy (TEM) with density functional theory (DFT) calculations. TEM images of the ALD Al2O3 overcoated Pd showed conformal Al2O3 films on...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Carbon
سال: 2014
ISSN: 0008-6223
DOI: 10.1016/j.carbon.2014.03.006