منابع مشابه
Laboratory evaluation of shear bond strength of porcelain repair methods
Introduction: Porcelain fracture is a relatively common problem in clinical dental practice. Various methods have been proposed for repairing porcelain fractures including direct composite resin repair or construction of a porcelain laminate veneer and its cementation with a resin cement. Evaluation of shear bond strength of porcelain repair methods was the purpose of this study. Methods: Tw...
متن کاملBond strength of chlorine peroxide.
The bond strength of chlorine peroxide (ClOOCl) is studied by photoionization mass spectrometry. The experimental results are obtained from the fragmentation threshold yielding ClO+, which is observed at 11.52 +/- 0.025 eV. The O-O bond strength D(o) is derived from this value in comparison to the first ionization energy of ClO, yielding D(o)298 = 72.39 +/- 2.8 kJ mol(-1). The present work prov...
متن کاملBond Strength of Orthodontic Adhesives
The objective of this study was to evaluate and compare bond strength of four adhesives used in orthodontics for bonding brackets to tooth enamel. The adhesives used in this investigation were resin-reinforced glass-ionomer cement (Fuji Ortho LC-GC Corporation, Japan), light cured composite resin adhesives (ConTec LC-Dentaurum, Germany and Enlight Bonding system-Ormco, USA) and dual cured compo...
متن کاملMicrotensile bond strength of clearfil SE bond to caries-affected dentin and normal dentin
Microtensile bond strength of clearfil SE bond to caries-affected dentin and normal dentin Dr. A. Ghasemi* - Dr. M. Bargrizan** - Dr. M. Mahmoodi*** *- Assistant Professor of Operative Dentistry Dept. - Faculty of Dentistry – Shaheed Beheshti University of Medical Sciences. **- Assistant Professor of Pedodontics Dept. - Faculty of Dentistry – Shaheed Beheshti University of Medical Sciences. ***...
متن کاملBond of High Strength Concrete with High Strength Reinforcing Steel
This paper presents a study about the bond of high strength concrete with high strength steel. Fourteen pull out tests were carried out to determine the bond. The concrete strength was about 70 MPa and the steel was a 500 MPa grade. Bar diameters used were 12, 16, 20, 25, 28, 32 and 36 mm. In order to investigate the effect of cover, each test was done twice, once in a 240 mm diameter concrete ...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: Sen-ito Kogyo
سال: 1970
ISSN: 1884-2275