Shear-based material removal processes significantly influence the quality of workpiece surface and implicitly component functional performance. An in-situ SEM nano-cutting enabled study crystal flow lattice rotation occurring below cutting edge in a polycrystalline Nickel superalloy. When within single grains deformed nanolayer appears that consists rotated exclusively plane which is delimited from bulk grain by high angle boundary (HAB); depth increases with pile-up (nano-chip) caused shearing. Upon multiple grains, nano-recrystallisation at HAB occurs, accompanied bending (GB) direction, phenomenon also influences deformation behaviour cut after passing GB. Clarifying these aspects nanoscale crucial for understanding formation damage operations.

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Effect of high temperature deformation on the structure of Ni based superalloy

Purpose: A study on the hot deformation behaviour and dynamic structural processes (dynamic precipitation operating during deformation at elevated temperatures) of nickel based superalloy was presented. Design/methodology/approach: Compression tests were carried out on precipitations hardenable nickel based superalloy of Inconel 718 at constant true strain rates of 10-4, 4x10-4s-1 within a temp...

متن کامل

the role of task-based techniques on the acquisition of english language structures by the intermediate efl students

this study examines the effetivenss of task-based activities in helping students learn english language structures for a better communication. initially, a michigan test was administered to the two groups of 52 students majoring in english at the allameh ghotb -e- ravandi university to ensure their homogeneity. the students scores on the grammar part of this test were also regarded as their pre...

15 صفحه اول

Nanoscale shear deformation mechanisms of opposing cartilage aggrecan macromolecules.

The nanoscale shear deformation behavior of two opposing end-grafted aggrecan layers was studied in aqueous solutions using atomic force microscopy, and was observed to depend markedly on bath ionic strength, the presence of calcium ions, and the applied lateral displacement rate. These results provide molecular-level insights into the contribution of aggrecan deformation mechanisms to cartilag...

متن کامل

study of hash functions based on chaotic maps

توابع درهم نقش بسیار مهم در سیستم های رمزنگاری و پروتکل های امنیتی دارند. در سیستم های رمزنگاری برای دستیابی به احراز درستی و اصالت داده دو روش مورد استفاده قرار می گیرند که عبارتند از توابع رمزنگاری کلیددار و توابع درهم ساز. توابع درهم ساز، توابعی هستند که هر متن با طول دلخواه را به دنباله ای با طول ثابت تبدیل می کنند. از جمله پرکاربردترین و معروف ترین توابع درهم می توان توابع درهم ساز md4, md...

Deformation compatibility in a single crystalline Ni superalloy

Deformation in materials is often complex and requires rigorous understanding to predict engineering component lifetime. Experimental understanding of deformation requires utilization of advanced characterization techniques, such as high spatial resolution digital image correlation (HR-DIC) and high angular resolution electron backscatter diffraction (HR-EBSD), combined with clear interpretatio...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Acta Materialia

سال: 2021

ISSN: ['1873-2453', '1359-6454']

DOI: https://doi.org/10.1016/j.actamat.2021.116929