Residual Stresses Analysis in Ball end Milling of Nickel-Based Superalloy Inconel 718

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

Investigation of Cutting Forces Superalloy Inconel 718

Since the cutting tools used in machining process of super alloys are subjected to high cutting forces, accordingly tools life is reduced, therefore improvement in alloys machining and reducing cutting forces to achieve longer tools life is an essential necessity. In this research, the effect of changes in feed rate on cutting forces in machining process of nickel based super alloys is investig...

متن کامل

Characterization of strain induced precipitation in Inconel 718 superalloy

Inconel 718 is a Ni-Cr-Fe superalloy which presents excellent mechanical properties at high temperatures, as well as good corrosion resistance and weldability. These characteristics can be optimized with an appropriate control of microstructural features such as grain size and precipitation. Precipitates of different nature can form in these alloys, i.e. γ’’ (a metastable metallic compound Ni3N...

متن کامل

Selective Growth of Low Stored Energy Grains During δ Sub-solvus Annealing in the Inconel 718 Nickel-Based Superalloy

The microstructure stability during d sub-solvus annealing in Inconel 718 was investigated, focusing on the conditions that may lead to the development of very large grains (about 100 lm) in a recrystallized fine grained matrix (4 to 5 lm) despite the presence of second-phase particles. Microstructure evolution was analyzed by EBSD (grain size, intragranular misorientation) and SEM (d phase par...

متن کامل

An Application of Computational Intelligence Technique for Predicting Surface Roughness in End Milling of Inconel-718

In this paper, an attempt has been made to design an computational intelligence technique based expert system using Adaptive Neuro-Fuzzy Inference System (ANFIS) for predicting surface roughness in end milling of Inconel 718. Two different types of membership functions are adopted for analysis in ANFIS training and compared their differences regarding the accuracy rate of the surface roughness ...

متن کامل

Analysis of Subsurface Microstructure and Residual Stresses in Machined Inconel 718 with PCBN and Al2O3-SiCw Tools

Subsurface microstructural alterations and residual stresses caused by machining significantly affect component lifetime and performance by influencing fatigue, creep, and stress corrosion cracking resistance. Assessing the surface quality of a machined part by characterizing subsurface microstructural alterations and residual stresses is essential for ensuring part performance and lifetime in ...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Materials Research

سال: 2017

ISSN: 1980-5373,1516-1439

DOI: 10.1590/1980-5373-mr-2017-0561