Reshaping nemato-elastic sheets.
We consider three-dimensional reshaping of thin nemato-elastic sheets containing half-charged defects upon nematic-isotropic transition. Gaussian curvature, that can be evaluated analytically when the nematic texture is known, differs from zero in the entire domain and has a dipole or hexapole singularity, respectively, at defects of positive or negative sign. The latter kind of defects appears...
متن کاملCapillary rise between elastic sheets
When a paintbrush is dipped into a pot of paint and pulled out, surface tension forces cause the individual hairs in the brush to coalesce even as the brush becomes impregnated with paint. We study a simple model of this elastocapillary interaction in the context of the surface-tension-driven vertical rise of a liquid between two long flexible hydrophilic sheets that are held a small distance a...
متن کاملStress focusing in elastic sheets
We review recent progress in understanding phenomena like crumpling, in which elastic membranes or sheets subject to structureless forces develop sharply curved structure over a small fraction of their surface. In the limit of zero thickness these structures become singular. After reviewing several related phenomena we note the physical elements that give rise to the singular behavior: elastici...
متن کاملImpacts on thin elastic sheets
We study transverse impacts of rigid objects on a free elastic membrane, using thin circular sheets of natural rubber as experimental models. After impact, two distinct axisymmetric waves propagate in and on the sheet. First a tensile wave travels at sound speed leaving behind the wave front a stretched domain. Then, a transverse wave propagates on the stretched area at a lower speed. In the st...
متن کاملCracking sheets: oscillatory fracture paths in thin elastic sheets.
When a blunt cutting tool is forced through a thin elastic sheet that is held along its lateral boundaries, a strikingly regular wavy cut can be left behind, examples of which are presented in Fig. 1. The thin film is brittle, hence it undergoes negligible irreversible deformation besides fracture. For tools much wider than the film’s thickness, the crack tip follows a highly reproducible nonsi...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: The European Physical Journal E
سال: 2015
ISSN: 1292-8941,1292-895X
DOI: 10.1140/epje/i2015-15075-6