Recent work in the creep field has indicated that the traditional methodologies involving power law equations are not sufficient to describe wide ranging creep behaviour. More recent approaches such as the Wilshire equations however, have shown promise in a wide range of materials, particularly in extrapolation of short term results to long term predictions. In the aerospace industry however, l...

متن کامل

A Coupled Creep-plasticity Model for Residual Stress Relaxation of a Shot-peened Nickel-base Superalloy

A COUPLED CREEP-PLASTICITY MODEL FOR RESIDUAL STRESS RELAXATION OF A SHOT-PEENED NICKEL-BASE SUPERALLOY Name: Dennis Justin Buchanan University of Dayton, 2007 Advisor: Dr. R. A. Brockman Shot peening has been employed in numerous industries for decades to impart beneficial compressive residual stresses on the surface of metal components. Compressive residual stresses retard initiation of surfa...

متن کامل

Joining of nickel-base superalloy single crystals

Introduction ................................................................................................................................1 Overview of Weldability of Nickel-Base Superalloys..................................................................1 Crystallography............................................................................................................................

متن کامل

Creep Crack Growth Simulation of Ni-base Superalloy

The purpose of this study is to develop a numerical approach to simulate the creep cracking of a Ni-base superalloy. The approach is based in continuum damage mechanics (CDM) and uses the classic Kachanov-Rabotnov constitutive equations for creep deformation and damage evolution. Creep damage takes the form of defects such as microcracks, cavities, voids, etc. A numerical crack growth algorithm...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Materials

سال: 2013

ISSN: 1996-1944

DOI: 10.3390/ma6031118