Quantitative Prediction of Embrittlement due to Pre-strain for Low Carbon Steels.

نویسندگان
چکیده

برای دانلود باید عضویت طلایی داشته باشید

برای دانلود متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

PREDICTION OF CRITICAL STRESS AND STRAIN FOR THE ONSET OF DYNAMIC RECRYSTALLIZATION IN PLAIN CARBON STEELS

The aim of the present study is the prediction of critical conditions (including critical strain and flow stress) for the initiation of dynamic recrystallization during thermo-mechanical processing of plain carbon steels. For this propose, torsion tests were conducted at different temperature (1050, 1100 and 1150˚C) and strain rates (0.002, 0.02 and 0.2/s). All flow curves showed a peak st...

متن کامل

an investication into the strain aging of low carbon steels

in this paper, the effect of prestrain on strain aging of low carbon steels, in the temperatures of 100°c and 200°c and the aging time of 50 minutes, and also the effect of aging temperature on strain aging in a constant aging time and prestrain, are investigated. the results of experiments show that with increasing the amount of prestrain, the increase in yield stress and ultimate tensile stre...

متن کامل

Application of Local Approach to Quantitative Prediction of Degradation in Fracture Toughness of Steels Due to Pre-Straining and Irradiation

Degradation of cleavage fracture toughness for low carbon steels due to pre-straining and irradiation was investigated on the basis of the local fracture criterion approach. Formulation of cleavage fracture toughness through the statistical modelling proposed by BEREMIN has been simplified by the present authors to the expression involving yield stress and cleavage fracture stress of materials....

متن کامل

Prevention of Hydrogen Embrittlement in Steels

The essential facts about the nature of the hydrogen embrittlement of steels have now been known for 140 years. It is diffusible hydrogen that is harmful to the toughness of iron. It follows, therefore, that the harmful influence of diffusible hydrogen can be mitigated by preventing its entry into steel or by rendering it immobile once it penetrates the material. This review deals with the meth...

متن کامل

Quantitative measuring of pearlite in carbon steels using electromagnetic sensor

Non-destructive Eddy current (EC) technique has long been used to detect discontinuities in materials. Recently, its application has been extended to characterize materials microstructure. In order to identify different microstructures, four plain carbon steel bars with different chemical compositions (AISI 1015, 1035, 1045 and 1080) were used in annealed condition. The pearlite percentage, car...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: QUARTERLY JOURNAL OF THE JAPAN WELDING SOCIETY

سال: 1996

ISSN: 0288-4771

DOI: 10.2207/qjjws.14.429