Protection of Crevice Corrosion of Titanium
نویسندگان
چکیده
منابع مشابه
Combining Rigorously Controlled Crevice Geometry and Computational Modeling for Study of Crevice Corrosion Scaling Factors
Microfabrication methods have been used to construct crevice formers of rigorously controlled gap and length. These have been used to study the IR-controlled crevice corrosion of Ni200 in 0.5 M H2SO4 to determine the effect of crevice gap ~G! on the position of the accelerated attack (xcrit) within the crevice. The experimental results were then compared to the results of computational studies....
متن کاملCombining the Ohmic Drop and Critical Crevice Solution Approaches to Rationalize Intermediate Attack in Crevice Corrosion
Crevice corrosion material loss is often most severe at intermediate distances into the crevice. This intermediate attack can be rationalized using the ohmic drop model of Pickering if and only if the material in question exhibits active/passive behavior in the crevice environment. Conventional theories that ascribe control of crevice corrosion to chemical changes exclusively cannot rationalize...
متن کاملVIII-Metals-J-Corrosion protection-1_ CORROSION PROTECTION OF METALS
Nearly all metals, with the exception of gold and platinum, will corrode in an oxidising environment forming compounds such as oxides, hydroxides and sulphides. The degradation of metals by corrosion is a universal reaction, caused by the simple fact that the oxide of a metal has a much lower energy than the metal itself. Hence there is a strong driving force for the oxidation of metals. For ex...
متن کاملBiofouling of Titanium – Biomineralization and Corrosion Aspects
Manganese oxidizing bacteria colonizing the titanium surfaces exposed to seawater were characterized by periodically retrieving the coupons over a period of two years. About 20% of the initial colonizers were capable of oxidizing manganese, and the dominant manganese oxidizing bacteria were those belonging to Gram negative Pseudomonas spp. Gram positive, Bacillus spp, were also observed, though...
متن کاملCorrosion of cemented titanium femoral stems.
Cemented titanium stems in hip arthroplasty are associated with proximal cement-stem ebonding and early failure. This was well publicised with the 3M Capital hip. However, corrosion in this setting has been reported with only one stem design and is less widely accepted. We present a series of 12 cemented titanium Furlong Straight Stems which required revision at a mean of 78 months for thigh pa...
متن کاملذخیره در منابع من
با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید
ژورنال
عنوان ژورنال: CORROSION ENGINEERING
سال: 1986
ISSN: 0010-9355,1884-1155
DOI: 10.3323/jcorr1974.35.9_538