Prediction of Primary Dendrite Arm Spacing with Solidification Velocity and Temperature Gradient during Directional Solidification in CMSX-4 Superalloy

نویسندگان
چکیده

برای دانلود رایگان متن کامل این مقاله و بیش از 32 میلیون مقاله دیگر ابتدا ثبت نام کنید

اگر عضو سایت هستید لطفا وارد حساب کاربری خود شوید

منابع مشابه

شببیه سازی تاثیر سرعت انجماد بر ریز ساختار آلیاژهای ریختگی آلومینیوم با استفاده از مدل شبکه عصبی مصنوعی

In cast aluminum and its alloys, the microstructure varies under different solidification conditions, causing variations in their mechanical properties. These materials are basically produced in sand and metallic molds or through die casting, each of which is associated with a unique solidification regime with significantly different cooling rates so that the resulting microstructure strongly d...

متن کامل

Cellular instabilities in directional solidification

2014 We have studied the morphology of the solid-liquid interface during the directional solidification of thin (5-150 03BCm) samples of a dilute binary mixture (CBr4/~ 0.1 % Br2) . Above a critical pulling speed, for a given temperature gradient and solute concentration, the interface, initially planar, breaks down into a periodic cellular pattern. The bifurcation from a planar to a cellular s...

متن کامل

Numerical Simulation and Optimization of Directional Solidification Process of Single Crystal Superalloy Casting

The rapid development of numerical modeling techniques has led to more accurate results in modeling metal solidification processes. In this study, the cellular automaton-finite difference (CA-FD) method was used to simulate the directional solidification (DS) process of single crystal (SX) superalloy blade samples. Experiments were carried out to validate the simulation results. Meanwhile, an i...

متن کامل

MODELLING OF THE PERMEABILITY FOR COLUMNAR DENDRITE STRUCTURES DURING SOLIDIFICATION OF MUSHY ALLOYS

A numerical model has been developed for the determination of liquid flow permeability through columnar dendrite during growth. The model is inclusive two stages, first numerical evolution of the dendrite shape during growth, and second numerical determination of the interdendritic liquid permeability. Simulation results shown which solute concentration by evolution of dendrite shape could resu...

متن کامل

Directional Solidification Microstructure of a Ni-Based Superalloy: Influence of a Weak Transverse Magnetic Field

A Ni-based superalloy CMSX-6 was directionally solidified at various drawing speeds (5–20 μm·s−1) and diameters (4 mm, 12 mm) under a 0.5 T weak transverse magnetic field. The results show that the application of a weak transverse magnetic field significantly modified the solidification microstructure. It was found that if the drawing speed was lower than 10 μm·s−1, the magnetic field caused ex...

متن کامل

ذخیره در منابع من


  با ذخیره ی این منبع در منابع من، دسترسی به آن را برای استفاده های بعدی آسان تر کنید

ژورنال

عنوان ژورنال: Korean Journal of Metals and Materials

سال: 2018

ISSN: 1738-8228,2288-8241

DOI: 10.3365/kjmm.2018.56.9.674